1-20 of 313 Search Results for

force measurement

Follow your search
Access your saved searches in your account

Would you like to receive an alert when new items match your search?
Close Modal
Sort by
Series: ASM Handbook
Volume: 11B
Publisher: ASM International
Published: 15 May 2022
DOI: 10.31399/asm.hb.v11B.a0006911
EISBN: 978-1-62708-395-9
.... In these tribometers, and the surfaces of the of polymers and counter-surfaces, there can be misalignment. Depending on the distance of sliding, this misalignment can be large enough to affect the measured friction forces and friction coefficient. In unidirectional sliding, this misalignment can be observed...
Series: ASM Failure Analysis Case Histories
Volume: 3
Publisher: ASM International
Published: 01 December 2019
DOI: 10.31399/asm.fach.v03.c9001762
EISBN: 978-1-62708-241-9
.... The pre-existing crack morphology was intergranular fracture in the axles studied. An estimate of the force required to cause the axle fracture can be made using the measured crack size, fracture toughness determined from these tests, and linear elastic fracture mechanics. The axle can be reliably said...
Series: ASM Failure Analysis Case Histories
Publisher: ASM International
Published: 01 June 2019
DOI: 10.31399/asm.fach.machtools.c0047779
EISBN: 978-1-62708-223-5
... Abstract Two A6 tool steel (free machining grade) shafts, parts of a clamping device used for bending 5.7 cm OD tubing on an 8.6 cm radius, failed simultaneously under a maximum clamping force of 54,430 kg. The shaft was imposed with cyclic tensile stresses due to the clamping force...
Series: ASM Failure Analysis Case Histories
Publisher: ASM International
Published: 01 June 2019
DOI: 10.31399/asm.fach.modes.c9001486
EISBN: 978-1-62708-234-1
... Abstract Cavitation damage of diesel engine cylinder liners is due to vibration of the cylinder wall, initiated by slap of the piston under the combined forces of inertia and firing pressure as it passes top dead center. The occurrence on the anti-thrust side may possibly result from bouncing...
Series: ASM Failure Analysis Case Histories
Publisher: ASM International
Published: 01 June 2019
DOI: 10.31399/asm.fach.auto.c0047846
EISBN: 978-1-62708-218-1
... loading. It was revealed by visual examination that the fracture had initiated in the sharp corner at the bottom of a longitudinal hole which was part of a force feed lubricating system. Beach marks were observed on the fracture surfaces. It was revealed by further examination that the slip clutch...
Series: ASM Handbook
Volume: 11B
Publisher: ASM International
Published: 15 May 2022
DOI: 10.31399/asm.hb.v11B.a0006930
EISBN: 978-1-62708-395-9
..., as it can be more sensitive than conventional torque data. As the technology of rheometers advances, normal force measurements will improve, and this parameter can be used more reliably to characterize polymer melts. Fig. 9 Rate sweep of PDMS (polydimethylsiloxane) with Parallel Plate (PP) geometry...
Series: ASM Handbook
Volume: 11B
Publisher: ASM International
Published: 15 May 2022
DOI: 10.31399/asm.hb.v11B.a0006919
EISBN: 978-1-62708-395-9
..., molded from a rubber-modified PC, was subjected to a dynamic force applied with the bar shown at the top of the figure ( Ref 5 ). Figure 8 illustrates the stress-strain response as a function of strain rate that was measured in standard tensile tests. Using a linear finite-element analysis...
Series: ASM Failure Analysis Case Histories
Publisher: ASM International
Published: 01 June 2019
DOI: 10.31399/asm.fach.aero.c0047076
EISBN: 978-1-62708-217-4
... notches, acting in combination with lateral forces evidenced by the moderate distortion of the fastener holes. Recommendations included eliminating the surface defects by revised cleaning and/or forming procedures. Revised design and installation should also alleviate the lateral forces. Aircraft...
Series: ASM Failure Analysis Case Histories
Publisher: ASM International
Published: 01 June 2019
DOI: 10.31399/asm.fach.design.c9001551
EISBN: 978-1-62708-233-4
... indicating rotational vibration fatigue. Keeping bolts tight solved this problem. In another case, grinding machines were unable to produce surfaces of uniform quality and smoothness on steel bearing products. Measurements showed that self-excited vibrations were created when particular steels were ground...
Series: ASM Failure Analysis Case Histories
Volume: 3
Publisher: ASM International
Published: 01 December 2019
DOI: 10.31399/asm.fach.v03.c9001759
EISBN: 978-1-62708-241-9
... the specified range of 58–62 RC; case depth achieved is also high. However, this causes through hardening at groove area of bearing cup, and hence, push-out force is less in the case of carburized and hardened samples compared with other samples, which was measured as 285 kg. Endurance test was found...
Series: ASM Handbook
Volume: 11B
Publisher: ASM International
Published: 15 May 2022
DOI: 10.31399/asm.hb.v11B.a0006932
EISBN: 978-1-62708-395-9
... of the type of deformation. In a study of nonlinear deformations and physical aging in PMMA, two researchers measured the torque and normal force in stress relaxation tests for different aging times ( Ref 57 ). They found that from 40 to 60 °C (105 to 140 °F), the aging curves for linear, small-strain...
Series: ASM Failure Analysis Case Histories
Volume: 3
Publisher: ASM International
Published: 01 December 2019
DOI: 10.31399/asm.fach.v03.c9001760
EISBN: 978-1-62708-241-9
.... As a result of these events, metallurgical investigations, fractography observation, finite element analysis, and some other measurements on failed cylinder head were conducted. Observation Results The cracked zone is shown in Fig. 1 . Checking the cooling and lubricating systems of the engine shows...
Series: ASM Handbook
Volume: 11B
Publisher: ASM International
Published: 15 May 2022
DOI: 10.31399/asm.hb.v11B.a0006910
EISBN: 978-1-62708-395-9
.... At greater load rates, for which no valid force-time signal for applying an FBA data reduction scheme can be recorded, the DKC method may be used to determine dynamic fracture toughness values. This requires an adequate technique to measure the time-to-fracture (e.g., specimens instrumented with crack tip...
Series: ASM Handbook
Volume: 11
Publisher: ASM International
Published: 15 January 2021
DOI: 10.31399/asm.hb.v11.a0006791
EISBN: 978-1-62708-295-2
... against each other at a constant speed, with the normal force gradually increasing during sliding. Twist Compression Test The twist compression test ( Fig. 15 ) uses the frictional force or coefficient of friction as the measured parameter that indicates adhesive failure or galling. As mentioned...
Series: ASM Failure Analysis Case Histories
Publisher: ASM International
Published: 01 June 2019
DOI: 10.31399/asm.fach.modes.c9001487
EISBN: 978-1-62708-234-1
... of the strip conductor due to centrifugal force. This leads to a high frictional binding force between turns and prevents axial expansion under normal heating in service. Rotor trouble which proved to be due to copper shortening was found in a set rated at 27.5 MW. It was manufactured in 1934 at which time...
Series: ASM Handbook
Volume: 11
Publisher: ASM International
Published: 15 January 2021
DOI: 10.31399/asm.hb.v11.a0006761
EISBN: 978-1-62708-295-2
..., test methods, temperature, and the nature of the applied stresses. In contrast, physical properties are those typically measured by methods not requiring the application of an external mechanical force (or load). Typical examples of physical properties are density, magnetic properties (e.g...
Series: ASM Handbook
Volume: 11B
Publisher: ASM International
Published: 15 May 2022
DOI: 10.31399/asm.hb.v11B.a0006928
EISBN: 978-1-62708-395-9
... and International Organization for Standardization (ISO) mechanical test standards for plastics ASTM International standard ISO standard Topic area of standard Specimen preparation D618 291 Methods of specimen conditioning D955 294-4 Measuring shrinkage from mold dimensions of molded...
Series: ASM Failure Analysis Case Histories
Publisher: ASM International
Published: 01 June 2019
DOI: 10.31399/asm.fach.bldgs.c9001576
EISBN: 978-1-62708-219-8
... operation. The casing of the fan was vibrated at 10 to 60 Hz. Peak stress easily overcame 30 MPa, which was enough to initiate cracking. The fracture surfaces and starting position were the same as those on the failed fan. It was concluded that the exciting force from an air compressor caused blade failure...
Series: ASM Failure Analysis Case Histories
Volume: 2
Publisher: ASM International
Published: 01 December 1993
DOI: 10.31399/asm.fach.v02.c9001287
EISBN: 978-1-62708-215-0
... was subjected to repeated tensile, compressive, and bending forces, had been machined from normalized stock without further treatment. Circumstances Leading to Failure The billet-loading tray on an industrial extrusion press is operated by two pneumatic rams. The pistons are mounted beneath the billet...
Series: ASM Failure Analysis Case Histories
Publisher: ASM International
Published: 01 June 2019
DOI: 10.31399/asm.fach.aero.c0006413
EISBN: 978-1-62708-217-4
... Abstract Examination of a 7075-T6 aluminum alloy pylon strut revealed cracks in two locations on the ears of the strut. Because the part was still intact, the cracks had to be forced open so that the fractures could be examined. Scanning electron microscopy (SEM) of the opened cracks showed...