EISBN: 978-1-62708-214-3
... diffraction analysis showed that the carbides were primarily chromium based (Cr 23 C 7 and Cr 7 C 3 ). The sooty substance was identified as graphite. Wasted areas were ferromagnetic and the degree of ferromagnetism was directly related to the degree of wastage. Three actions were recommended: (1) inspection...
Series: ASM Failure Analysis Case Histories
Publisher: ASM International
Published: 01 June 2019
DOI: 10.31399/asm.fach.process.c9001581
EISBN: 978-1-62708-235-8
... stainless steels, such as alloys 304L, 304, and 304H, have essentially no ferromagnetic phases when they are in the solution annealed condition. Cold work causes a partial transformation to martensite and causes the structure to show a ferromagnetic response. The martensite reverts to austenite on annealing...
Series: ASM Failure Analysis Case Histories
Publisher: ASM International
Published: 01 June 2019
DOI: 10.31399/asm.fach.aero.c0089563
EISBN: 978-1-62708-217-4
... of a casting, magnetic-particle inspection is a relatively reliable method of detecting them in ferromagnetic materials. The following contributors provided case histories or other useful information to the source article: Charles O. Cambridge, Navistar International, Inc.; George M. Goodrich, Taussig...
Series: ASM Failure Analysis Case Histories
Publisher: ASM International
Published: 01 June 2019
DOI: 10.31399/asm.fach.power.c9001661
EISBN: 978-1-62708-229-7
... on the results of the evaluation program. This procedure is applicable to the magnetic particle examination of ferromagnetic components using prods and dry powder with direct current (DC) according to the dry continuous inspection method. This procedure is limited to the detection of discontinuities open...
Series: ASM Handbook
Volume: 11
Publisher: ASM International
Published: 15 January 2021
DOI: 10.31399/asm.hb.v11.a0006758
EISBN: 978-1-62708-295-2
... are potential NDE options. For example, MT is useful for ferromagnetic materials but not for nonferromagnetic materials. Electrical conductivity, resistivity, and dielectric properties may be needed to determine inspection feasibility and for calibration purposes. Part thickness and density are important...
Series: ASM Handbook Archive
Volume: 11
Publisher: ASM International
Published: 01 January 2002
DOI: 10.31399/asm.hb.v11.a0003515
EISBN: 978-1-62708-180-1
... that can be magnetized (ferromagnetic) to detect surface or near-surface discontinuities. Relatively easy to use. Portable equipment is available for field testing. Cannot be used on metals that cannot be magnetized. Requires properly trained personnel with considerable application experience...
Series: ASM Handbook
Volume: 11A
Publisher: ASM International
Published: 30 August 2021
DOI: 10.31399/asm.hb.v11A.a0006808
EISBN: 978-1-62708-329-4
Series: ASM Handbook
Volume: 11
Publisher: ASM International
Published: 15 January 2021
DOI: 10.31399/asm.hb.v11.a0006764
EISBN: 978-1-62708-295-2
...-particle inspection (MPI) uses magnetic fields to locate surface and subsurface discontinuities in ferromagnetic materials. When the material or part to be tested is magnetized, discontinuities that generally lie transverse to the direction of the magnetic field will cause a leakage field to be formed...
Series: ASM Handbook Archive
Volume: 11
Publisher: ASM International
Published: 01 January 2002
DOI: 10.31399/asm.hb.v11.a0003524
EISBN: 978-1-62708-180-1
... of nondestructive inspection is a necessary part of record keeping in the investigation. Magnetic-Particle Inspection Magnetic-particle inspection utilizes magnetic fields to locate surface and subsurface discontinuities in ferromagnetic materials. When the material or part to be tested is magnetized...
Series: ASM Failure Analysis Case Histories
Publisher: ASM International
Published: 01 June 2019
DOI: 10.31399/asm.fach.modes.c9001459
EISBN: 978-1-62708-234-1
Series: ASM Handbook
Volume: 11A
Publisher: ASM International
Published: 30 August 2021
DOI: 10.31399/asm.hb.v11A.a0006830
EISBN: 978-1-62708-329-4
... for Electromagnetic Examination of Ferromagnetic Steel Wire Rope ,” E 1571-11(2016)e1, ASTM International , West Conshohocken, PA , 2016 , www.astm.org 4. “ Standard Specification for Carbon Steel Chain ,” A 413/A 413M-07(2012), ASTM International , West Conshohocken, PA , 2012 , www.astm.org 5...
Series: ASM Handbook
Volume: 11A
Publisher: ASM International
Published: 30 August 2021
DOI: 10.31399/asm.hb.v11A.a0006810
EISBN: 978-1-62708-329-4
Series: ASM Handbook
Volume: 11A
Publisher: ASM International
Published: 30 August 2021
DOI: 10.31399/asm.hb.v11A.a0006825
EISBN: 978-1-62708-329-4
Series: ASM Handbook Archive
Volume: 11
Publisher: ASM International
Published: 01 January 2002
DOI: 10.31399/asm.hb.v11.a0003508
EISBN: 978-1-62708-180-1