Series: ASM Failure Analysis Case Histories
Volume: 1
Publisher: ASM International
Published: 01 December 1992
DOI: 10.31399/asm.fach.v01.c9001107
EISBN: 978-1-62708-214-3
... of the waste heat boiler to determine the extent of metal damage in other areas by measuring the degree of ferromagnetism, (2) replacement of metal determined to be magnetic, and (3) closer monitoring of temperatures in the region of the reformer furnace outlet. Boilers Chemical processing equipment...
Series: ASM Failure Analysis Case Histories
Publisher: ASM International
Published: 01 June 2019
DOI: 10.31399/asm.fach.process.c9001581
EISBN: 978-1-62708-235-8
... for Metals , Metals Park, OH , 1977 , p. 373 . 4. An Evaluation of the Yield, Tensile, Creep, and Rupture Strengths of Wrought 304, 316, 321, and 347 Stainless Steels at Elevated Temperatures , ASTM Data Series DS-5S2 , ASTM , Philadelphia, PA , 1969 . Selected Reference Selected Reference...
Series: ASM Failure Analysis Case Histories
Publisher: ASM International
Published: 01 June 2019
DOI: 10.31399/asm.fach.aero.c0089563
EISBN: 978-1-62708-217-4
... that the lever had broken at a cold shut ( Fig. 1 ) that extended through about 95% of the cross section of the lever arm. The remaining 5% of the cross section appeared to be sound metal. Specifications for both the casting and the finished lever required radiographic inspection. This inspection method...
Series: ASM Failure Analysis Case Histories
Publisher: ASM International
Published: 01 June 2019
DOI: 10.31399/asm.fach.power.c9001661
EISBN: 978-1-62708-229-7
... evaluation of these discontinuities, analysis of the failure modes and determination of the best repair techniques. A recommended resolution of the problem was to be prepared based on the results of the evaluation program. This procedure is applicable to the magnetic particle examination of ferromagnetic...
Series: ASM Handbook
Volume: 11
Publisher: ASM International
Published: 15 January 2021
DOI: 10.31399/asm.hb.v11.a0006758
EISBN: 978-1-62708-295-2
... into the volume of the component. NDE techniques such as eddy current testing (ET) for electrically-conductive materials, full volumetric inspection using ultrasonic testing (UT) for metals, and radiographic testing (RT) are available in these instances. Eddy current testing is typically only able...
Series: ASM Handbook Archive
Volume: 11
Publisher: ASM International
Published: 01 January 2002
DOI: 10.31399/asm.hb.v11.a0003515
EISBN: 978-1-62708-180-1
... applied to the surface indicate the location of a field leakage, signaling a discontinuity. Used on metal that can be magnetized (ferromagnetic) to detect surface or near-surface discontinuities. Relatively easy to use. Portable equipment is available for field testing. Cannot be used on metals...
Series: ASM Handbook
Volume: 11
Publisher: ASM International
Published: 15 January 2021
DOI: 10.31399/asm.hb.v11.a0006764
EISBN: 978-1-62708-295-2
... examination of large areas. Can be adapted to production inspections Circuit board solder joints, solar cells, heat-transfer equipment, metals, composites, concrete Sonic IR/vibro-thermography, inductive IR Acoustic or inductive energy is applied to a part, and cracks heat up more than surrounding...
Series: ASM Handbook Archive
Volume: 11
Publisher: ASM International
Published: 01 January 2002
DOI: 10.31399/asm.hb.v11.a0003524
EISBN: 978-1-62708-180-1
... in portable testers. The major components of the portable laboratory may include: A custom-made machine, plus auxiliary materials, for grinding and polishing small, mounted or unmounted metal specimens A right-angle head, electric drill motor with attachments and materials for grinding...
Series: ASM Failure Analysis Case Histories
Publisher: ASM International
Published: 01 June 2019
DOI: 10.31399/asm.fach.modes.c9001459
EISBN: 978-1-62708-234-1
...—New Series , Vol. I , p. 103 . 5. Ibid , p. 114 . 6. Bacon F. , Engineering , Sept . 23rd , 1932 , p. 372 . 7. Peterson R. E. , “Metals and Alloys,” Vol. 10 , 1939 , p. 276 . 8. “Handbook of Experimental Stress Analysis,” 1950 ( John Wiley & Sons Inc...
Series: ASM Handbook Archive
Volume: 11
Publisher: ASM International
Published: 01 January 2002
DOI: 10.31399/asm.hb.v11.a0003508
EISBN: 978-1-62708-180-1
..., Table 1 ): Metallic projections Cavities Discontinuities Defects Incomplete casting Incorrect dimension Inclusions or structural anomalies Table 1 International classification of common casting defects No. Description Common name Sketch Metallic Projections...