1-20 of 417 Search Results for

failure modes and effects analysis

Follow your search
Access your saved searches in your account

Would you like to receive an alert when new items match your search?
Close Modal
Sort by
Series: ASM Handbook Archive
Volume: 11
Publisher: ASM International
Published: 01 January 2002
DOI: 10.31399/asm.hb.v11.a0003503
EISBN: 978-1-62708-180-1
... Abstract This article describes the methodology for performing a failure modes and effects analysis (FMEA). It explains the methodology with the help of a hot water heater and provides a discussion on the role of FMEA in the design process. The article presents the analysis procedures and shows...
Series: ASM Handbook
Volume: 11A
Publisher: ASM International
Published: 30 August 2021
DOI: 10.31399/asm.hb.v11A.a0006817
EISBN: 978-1-62708-329-4
... process. It then expands on questions involved in RCM process, offering definitions when necessary. Next, the article describes the approach of RCM to failure modes and effects analysis (FMEA), the failure management policies available under RCM, and the criteria of RCM for deciding when a specific...
Series: ASM Handbook Archive
Volume: 11
Publisher: ASM International
Published: 01 January 2002
DOI: 10.31399/asm.hb.v11.a0003504
EISBN: 978-1-62708-180-1
... modes and effects analysis (FMEA), and therefore, the article explains the approach of RCM to FMEA and the failure management policies available under RCM. It reviews the ways that RCM classifies failure effects in terms of consequences and details how RCM uses failure consequences to identify the best...
Series: ASM Handbook
Volume: 11A
Publisher: ASM International
Published: 30 August 2021
DOI: 10.31399/asm.hb.v11A.a0006815
EISBN: 978-1-62708-329-4
... of failure. Next, the article discusses the steps involved in the engineering design process and explains the importance of considering the engineering design process. Information on failure modes and effects analysis is also provided. The article ends with a discussion on the consequence of management...
Series: ASM Handbook Archive
Volume: 11
Publisher: ASM International
Published: 01 January 2002
DOI: 10.31399/asm.hb.v11.9781627081801
EISBN: 978-1-62708-180-1
Series: ASM Handbook
Volume: 11B
Publisher: ASM International
Published: 15 May 2022
DOI: 10.31399/asm.hb.v11B.a0006945
EISBN: 978-1-62708-395-9
... uorinated ethylene propylene ame ionization detector failure modes and effects analysis exible PVC ber-reinforced polymer (or plastic) Fourier transform infrared spectroscopy glass reinforced epoxy resin glass ber glass ber reinforced polymer (or plastic) gel permeation chromatography high-density...
Series: ASM Handbook Archive
Volume: 11
Publisher: ASM International
Published: 01 January 2002
DOI: 10.31399/asm.hb.v11.a0006548
EISBN: 978-1-62708-180-1
... appearance transition tempera- ture fcc face-centered cubic FCAW flux cored arc welding FDA Food and Drug Administration FEA finite element analysis FFS fit for service FHA fault hazard analysis Fig. figure FMEA failure modes and effects analysis FMECA failure modes, effects, and criticality analysis FRP...
Series: ASM Handbook
Volume: 11B
Publisher: ASM International
Published: 15 May 2022
DOI: 10.31399/asm.hb.v11B.a0006942
EISBN: 978-1-62708-395-9
... Material Selection Manufacturing Process Failure Modes and Effects Analysis The Failure Analysis Process Five Whys Misuse Service-Related Incidents End of Life Why Perform a Failure Analysis? Nondestructive Examination Obtain Background Information Fishbone Diagram...
Series: ASM Handbook
Volume: 11
Publisher: ASM International
Published: 15 January 2021
DOI: 10.31399/asm.hb.v11.a0006758
EISBN: 978-1-62708-295-2
... particle testing. It covers the effects of various factors on the properties of the part that may impact failure analysis, describes the characterization of damage modes and crack sizes, and finally discusses the processes involved in application of NDE results to failure analysis. crack sizes...
Series: ASM Handbook
Volume: 11
Publisher: ASM International
Published: 15 January 2021
DOI: 10.31399/asm.hb.v11.a0006753
EISBN: 978-1-62708-295-2
..., and material, which are discussed in the following sections along with examples. The tools available for failure analysis are then covered. Further, the article describes the categories of mode of failure: distortion or undesired deformation, fracture, corrosion, and wear. It provides information...
Series: ASM Failure Analysis Case Histories
Publisher: ASM International
Published: 01 June 2019
DOI: 10.31399/asm.fach.power.c9001561
EISBN: 978-1-62708-229-7
... and weld material, in addition to fractography, EPR testing and optical microscopy in discerning the mode of failure. Various effects of Cl-, O2 and MnS are discussed. Results indicated that the cause of failure was the severe sensitization coupled with probable contamination by S and possibly by Cl ions...
Series: ASM Handbook Archive
Volume: 11
Publisher: ASM International
Published: 01 January 2002
DOI: 10.31399/asm.hb.v11.a0003519
EISBN: 978-1-62708-180-1
... or as an individual. The Failsafe system also includes the Combing Process, a failure mode and effects analysis (FMEA)-based tool for rapidly identifying “significant few” chronic failures in hours or days. It proposes to be an approach that goes to the hands-on operating and maintenance people for information...
Series: ASM Handbook
Volume: 11B
Publisher: ASM International
Published: 15 May 2022
DOI: 10.31399/asm.hb.v11B.a0006919
EISBN: 978-1-62708-395-9
... it.. It describes the effects of loading rate on polymer deformation and the influence of temperature and strain rate on failure mode. It discusses the advantages and limitations of standard impact tests, the use of puncture tests for assessing material behavior under extreme strain, and the application of fracture...
Series: ASM Handbook Archive
Volume: 11
Publisher: ASM International
Published: 01 January 2002
DOI: 10.31399/asm.hb.v11.a0003500
EISBN: 978-1-62708-180-1
... (RCA) techniques are effective in exploring some of the other contributors to failures, such as the human and latent root causes. Properly performed, failure analysis and RCA are critical steps in the overall problem-solving process and are key ingredients for correcting and preventing failures...
Series: ASM Failure Analysis Case Histories
Publisher: ASM International
Published: 01 June 2019
DOI: 10.31399/asm.fach.usage.c9001672
EISBN: 978-1-62708-236-5
... spring fracture surface at the crack origin of the longitudinal defect; and, (d) SEM view of a secondary crack or crack branching. Fractographic analysis of the spring fracture surfaces revealed a corroded morphology as can be seen in Figure 3 . No clear evidence of the mode of failure could...
Series: ASM Failure Analysis Case Histories
Publisher: ASM International
Published: 01 June 2019
DOI: 10.31399/asm.fach.conag.c9001500
EISBN: 978-1-62708-221-1
... of the two intact teeth in the spiral bevel pinion shown in Fig. 1 . Note the altered martensite in the subsurface shear plane. These “butterfly wings” extended from 0.010 to 0.035 in. below the surface. Final Analysis The mode of failure is rolling contact fatigue, and the cause of failure...
Series: ASM Failure Analysis Case Histories
Publisher: ASM International
Published: 01 June 2019
DOI: 10.31399/asm.fach.modes.c9001394
EISBN: 978-1-62708-234-1
... that failure resulted from an intergranular attack. Subsequent microscope examination confirmed the generally intergranular mode of failure. A macro-etched section near the fracture revealed a radial arrangement of columnar crystals, indicating that the spindle was a cast and not a wrought product as had been...
Series: ASM Failure Analysis Case Histories
Volume: 3
Publisher: ASM International
Published: 01 December 2019
DOI: 10.31399/asm.fach.v03.c9001841
EISBN: 978-1-62708-241-9
... Selected References • James B.A. , Medical Device Failure Analysis , Materials for Medical Devices , Vol 23 , ASM Handbook , Narayan R.J. , Ed., ASM International , 2012 , p 343 – 359 . 10.31399/asm.hb.v23.a0005657 • T. Service , Finite Element Modeling in Failure...
Series: ASM Failure Analysis Case Histories
Volume: 2
Publisher: ASM International
Published: 01 December 1993
DOI: 10.31399/asm.fach.v02.c9001377
EISBN: 978-1-62708-215-0
... of this analysis is represented in Fig. 15 , 16 , 17 , which illustrate the mode of H 2 S stress-corrosion cracking propagation. Cracking originated at the bolt shank surface and progressed inward slowly along an intergranular path, accompanied by secondary cracks. When the effective cross section could...
Series: ASM Handbook Archive
Volume: 11
Publisher: ASM International
Published: 01 January 2002
DOI: 10.31399/asm.hb.v11.a0005695
EISBN: 978-1-62708-180-1
.... It is defined within ASME Failure Methods and Effects Analysis terminology, and there are some eight additional definitions in Webster's Unabridged Dictionary. There are still more uses of the term, as in fracture mode, failure mode , and so on. These latter two terms are not in the ASM Materials...