Published: 01 June 2019
Fig. 7 Decarburization on the surface of spring leg. Etchant, 2 pct Nital. Magnification 82 times. More
Image
Published: 01 June 2019
Fig. 1 Core structure of the wires. G. Cross sections, etchant: picral. 200 × More
Image
Published: 01 June 2019
Fig. 2 Cross sections, etchant: picral. 200 × Core structure of the wires. S1. More
Image
Published: 01 June 2019
Fig. 3 Cross sections, etchant: picral. 200 × Core structure of the wires. S2. More
Image
Published: 01 June 2019
Fig. 4 Cross sections, etchant: picral. 200 × Edge structure of the wires. S1. More
Image
Published: 01 June 2019
Fig. 5 Cross sections, etchant: picral. 200 × Edge structure of the wires. S2. More
Image
Published: 01 June 2019
Fig. 6 Cross sections, etchant: picral. 200 × Edge structure of the wires. G. More
Image
Published: 01 June 2019
Fig. 2 Structure after heat-treatment, etchant: Picral. 100× More
Image
Published: 01 June 2019
Fig. 2 Longitudinal section through the weld. Etchant: Nital. 8 × More
Image
Published: 01 June 2019
Fig. 4 Microstructure of the mild steel pipe, etchant: Picral. 100 × More
Image
Published: 01 June 2019
Fig. 5 Microstructure of the welding material, etchant: V2A-etching solution. 500 × More
Image
Published: 01 June 2019
Fig. 6 Microstructure of the chrome steel pipe, etchant: V2A-etching solution. 500 × More
Image
Published: 01 June 2019
Fig. 7 Microstructure of the transition zone, etchant: V2A-etching solution. 100 × More
Image
Published: 01 June 2019
Fig. 6 Course of crack in microstructure; etchant: copper ammonium chloride ammonium hydroxide. 100× More
Image
Published: 01 June 2019
Fig. 3 Longitudinal section s—s in Fig. 2 through a hard spot. Etchant: Nital. 10 × More
Image
Published: 01 June 2019
Fig. 4 Microstructure in the weldseam, longitudinal section. Etchant: Nital. 500 ×. Normal location. More
Image
Published: 01 June 2019
Fig. 5 Microstructure in the weldseam, longitudinal section. Etchant: Nital. 500 ×. Carburized locations. Hypo-eutectoid. More
Image
Published: 01 June 2019
Fig. 6 Microstructure in the weldseam, longitudinal section. Etchant: Nital. 500 ×. Carburized locations. Near-eutectoid. More
Image
Published: 01 June 2019
Fig. 7 Microstructure in the weldseam, longitudinal section. Etchant: Nital. 500 ×. Carburized locations. Hyper-eutectoid. More