Series: ASM Failure Analysis Case Histories
Publisher: ASM International
Published: 01 June 2019
DOI: 10.31399/asm.fach.petrol.c9001603
EISBN: 978-1-62708-228-0
.... , Edwards P.D. , and Kelly P.G. : Int. Conf. Thermomechanical Processing of Steels and Other Materials, Thermec ’97 , TMS , Australia , 1997 , pp. 475 – 82 . 5. Ramaswamy V. , Datta R. , Chaudhuri S.K. , and Mishra S. : Proc. Symp. Emerging Technologies for New...
Series: ASM Handbook Archive
Volume: 11
Publisher: ASM International
Published: 01 January 2002
DOI: 10.31399/asm.hb.v11.a0003532
EISBN: 978-1-62708-180-1
...) abrasive embedded in the surface of a partly prepared specimen of lead Fig. 34 Light micrograph of a grossly overaustenitized AISI D2 draw die insert. Specimen etched with Marble's reagent Fig. 35 Light micrographs showing (a) planar and (b) through-thickness views of cracking...
Series: ASM Handbook
Volume: 11A
Publisher: ASM International
Published: 30 August 2021
DOI: 10.31399/asm.hb.v11A.a0006816
EISBN: 978-1-62708-329-4
...) Presence of scale or decarburization Grinding stresses Localized stresses If abusive, localized martensitic microstructures Surface tensile stress, with subsurface compressive component Shot and grit blasting Localized surface stresses Very shallow and compressive surface...
Series: ASM Handbook
Volume: 11A
Publisher: ASM International
Published: 30 August 2021
DOI: 10.31399/asm.hb.v11A.a0006826
EISBN: 978-1-62708-329-4
... of Aluminum Alloys , Aluminum Science and Technology , Vol 2A , ASM Handbook , ASM International , 2018 , p 508 10.31399/asm.hb.v02a.a0006494 18. Ezugwu E.O. , Key Improvements in the Machining of Difficult-to-Cut Aerospace Superalloys , Int. J. Mach. Tools Manuf. , Vol 45 , 2005 , p...
Series: ASM Handbook Archive
Volume: 11
Publisher: ASM International
Published: 01 January 2002
DOI: 10.31399/asm.hb.v11.a0003507
EISBN: 978-1-62708-180-1
... internal quality due to compressive deformation Grain refinement Uniform grain structure Elimination of casting porosity and breakup of macrosegregation patterns Beneficial grain-flow pattern for improved part performance Improved toughness and/or fatigue resistance due to grain flow...
Series: ASM Handbook
Volume: 11A
Publisher: ASM International
Published: 30 August 2021
DOI: 10.31399/asm.hb.v11A.a0006837
EISBN: 978-1-62708-329-4
... the corrosion material embedded in some of the pits Fig. 39 Secondary fatigue cracks present near primary fracture surface Fig. 50 As-received wheelset with portion missing Fig. 51 As-received rim sections viewed from the back rim face. Circled area indicates initiation region...
Series: ASM Handbook Archive
Volume: 11
Publisher: ASM International
Published: 01 January 2002
DOI: 10.31399/asm.hb.v11.a0003530
EISBN: 978-1-62708-180-1
... and compressive failure stresses), anisotropic behavior and nonconstancy of volume during deformation. The historically early models (Rankine, Tresca, von Mises, and octahedral shear) were phenomenological and as proposed could be applied to either failure by yield or failure by fracture. They have also been...
Series: ASM Handbook
Volume: 11
Publisher: ASM International
Published: 15 January 2021
DOI: 10.31399/asm.hb.v11.a0006767
EISBN: 978-1-62708-295-2
... based on maximum strain). Additionally, some criteria take into account polar behavior (unequal tensile and compressive failure stresses), anisotropic behavior, and nonconstancy of volume during deformation. The historically early models (Rankine, Tresca, von Mises, and octahedral shear) were...
Series: ASM Handbook
Volume: 11A
Publisher: ASM International
Published: 30 August 2021
DOI: 10.31399/asm.hb.v11A.a0006811
EISBN: 978-1-62708-329-4
.... , Compressive Damage-Induced Cracking in Nitinol , SMST-2004: Proceedings of the International Conference on Shape Memory and Superelastic Technologies , 2006 , p 117 91. “Standard Specification and Test Method for Metallic Bone Plates,” F 382, Annual Book of ASTM Standards , American Society...
Series: ASM Handbook Archive
Volume: 11
Publisher: ASM International
Published: 01 January 2002
DOI: 10.31399/asm.hb.v11.a0003560
EISBN: 978-1-62708-180-1
... 10.1016/0043-1648(81)90062-4 22. Hutchings I.M. , Tribology: Friction and Wear of Engineering Materials , CRC Press , 1992 23. Kosel T.H. , Solid Particle Erosion , Friction, Lubrication, and Wear Technology , Vol 18 , ASM Handbook , Blau P.J. , Ed., ASM...
Series: ASM Handbook
Volume: 11A
Publisher: ASM International
Published: 30 August 2021
DOI: 10.31399/asm.hb.v11A.9781627083294
EISBN: 978-1-62708-329-4
Book Chapter

Series: ASM Handbook
Volume: 11
Publisher: ASM International
Published: 15 January 2021
DOI: 10.31399/asm.hb.v11.a0006790
EISBN: 978-1-62708-295-2
... , Wear , Vol 65 , 1981 , p 359 – 373 10.1016/0043-1648(81)90062-4 22. Hutchings I.M. , Tribology: Friction and Wear of Engineering Materials , CRC Press , 1992 23. Kosel T.H. , Solid Particle Erosion , Friction, Lubrication, and Wear Technology , Vol 18 , ASM Handbook...
Series: ASM Handbook
Volume: 11A
Publisher: ASM International
Published: 30 August 2021
DOI: 10.31399/asm.hb.v11A.a0006834
EISBN: 978-1-62708-329-4
... 18 Fig. 4 Distribution of required hardness within the thickness of the material (it follows the maximum shear stress, τ shear , below the surface) under normal compressive load, F compr (most loaded rolling element), where curve 1 is shear stress, τ shear , and curve 2 is material...
Series: ASM Handbook Archive
Volume: 11
Publisher: ASM International
Published: 01 January 2002
DOI: 10.31399/asm.hb.v11.a0003524
EISBN: 978-1-62708-180-1
... for direct, nondestructive measurement of residual (internal) stresses in metals. Stresses are determined by measuring the submicroscopic distortion of crystalline lattice structures by tensile or compressive residual stresses. However, it should be pointed out that measurement of residual stresses near...
Series: ASM Handbook
Volume: 11A
Publisher: ASM International
Published: 30 August 2021
DOI: 10.31399/asm.hb.v11A.a0006822
EISBN: 978-1-62708-329-4
... Report OPS 89-1, Office of Pipeline Safety , U.S. Department of Transportation , Aug 1989 7. Quickel G.T. , Rollins B.C. , and Beavers J.A. , Analysis of Seam Weld Related Pipeline Failures , Failure Analysis for Problem Solving, Materials Science & Technology Conference...
Series: ASM Handbook
Volume: 11A
Publisher: ASM International
Published: 30 August 2021
DOI: 10.31399/asm.hb.v11A.a0006838
EISBN: 978-1-62708-329-4
... MANUFACTURING (AM) refers to a group of free-form fabrication technologies that incrementally build up a solid part by computer-controlled deposition of material from a digital solid model. The technology is an outgrowth and broadening of rapid prototyping methods that were developed in the 1980s to accelerate...
Series: ASM Handbook
Volume: 11A
Publisher: ASM International
Published: 30 August 2021
DOI: 10.31399/asm.hb.v11A.a0006819
EISBN: 978-1-62708-329-4
.... An overview of high-cycle welded fatigue methods, cycle-counting techniques, and a discussion on ratcheting are also offered. A historical synopsis of fatigue technology advancements and commentary on component design and fabrication strategies to mitigate fatigue damage and improve damage tolerance...
Series: ASM Handbook Archive
Volume: 11
Publisher: ASM International
Published: 01 January 2002
DOI: 10.31399/asm.hb.v11.a0003508
EISBN: 978-1-62708-180-1
... angles and cores) Metal penetration D 224 Fragment of mold material embedded in casting surface Dip coat spall, scab D 230: Plate-like metallic projections with rough surfaces, usually parallel to casting surface D 231 (a) Plate-like metallic projections with rough surfaces...
Series: ASM Handbook
Volume: 11A
Publisher: ASM International
Published: 30 August 2021
DOI: 10.31399/asm.hb.v11A.a0006831
EISBN: 978-1-62708-329-4
... and metal at the hottest points of the casting (re-entrant angles and cores) Metal penetration D 224 Fragment of mold material embedded in casting surface Dip coat spall, scab D 230 Plate-like metallic projections with rough surfaces, usually parallel to casting surface D 231...
Series: ASM Handbook Archive
Volume: 11
Publisher: ASM International
Published: 01 January 2002
DOI: 10.31399/asm.hb.v11.a0003522
EISBN: 978-1-62708-180-1
... for include the nature of the damage, for example, overall wear or scores in the bearing surfaces. In the latter case, it is particularly important to identify any hard particles that may be embedded and trapped at the ends of the score marks. Where unexpected wear between components in relative motion...