1-3 of 3 Search Results for

electronics and telecommunications

Sort by
Series: ASM Handbook
Volume: 11B
Publisher: ASM International
Published: 15 May 2022
DOI: 10.31399/asm.hb.v11B.a0006939
EISBN: 978-1-62708-395-9
... Abstract Polymer materials are key building blocks of the modern world, commonly used in packaging, automobiles, building materials, electronics, telecommunications, and many other industries. These commercial applications of polymeric materials would not be possible without the use...
Series: ASM Failure Analysis Case Histories
Volume: 3
Publisher: ASM International
Published: 01 December 2019
DOI: 10.31399/asm.fach.v03.c9001843
EISBN: 978-1-62708-241-9
... not be any issues, since they rarely are exposed to temperatures below 55 °F. So your average TV, DVD player, and Wii are going to be unaffected. But what may be more susceptible are electronic products destined to operate in cold climates, like telecommunication base stations (cell phone towers...
Series: ASM Handbook
Volume: 11B
Publisher: ASM International
Published: 15 May 2022
DOI: 10.31399/asm.hb.v11B.a0006925
EISBN: 978-1-62708-395-9
... as the backbone of most polymers, tend to result in lower density relative to metals and ceramics. The localized nature of electrons in polymers also renders them good electrical insulators and poor thermal conductors. Bond energies for various materials Table 2 Bond energies for various materials...