1-20 of 231 Search Results for

electrical measurement

Follow your search
Access your saved searches in your account

Would you like to receive an alert when new items match your search?
Close Modal
Sort by
Series: ASM Failure Analysis Case Histories
Publisher: ASM International
Published: 01 June 2019
DOI: 10.31399/asm.fach.mech.c0047935
EISBN: 978-1-62708-225-9
... in the bearings was suspected to have caused the electric discharge by accumulation and discharge of static charge. The electrical resistance between the rotor and the motor frame lubricated with electrically conductive grease and the grease used in the current case was measured and compared to confirm the fact...
Series: ASM Failure Analysis Case Histories
Publisher: ASM International
Published: 01 June 2019
DOI: 10.31399/asm.fach.usage.c0047823
EISBN: 978-1-62708-236-5
... stresses were caused by misalignment between the electric motor and compressor and were transmitted to the shaft through the geared coupling. Flexible-disk couplings capable of transmitting the required horsepower were installed on the shafts as a corrective measure. Alignment Bending Radii 4340...
Series: ASM Failure Analysis Case Histories
Publisher: ASM International
Published: 01 June 2019
DOI: 10.31399/asm.fach.mech.c0048139
EISBN: 978-1-62708-225-9
... striations within the beach-mark regions were revealed by scanning electron microscopy. As a corrective measure, the spring-winding operation was altered to eliminate the tool marks. Electrical switches Winding 302 UNS S30200 Fatigue fracture Several electrical toggle switches failed...
Series: ASM Failure Analysis Case Histories
Volume: 1
Publisher: ASM International
Published: 01 December 1992
DOI: 10.31399/asm.fach.v01.c9001116
EISBN: 978-1-62708-214-3
...Abstract Abstract Two failures of AP15A grade J-55 electric resistance welded (ERW) tubing in as our gas environment were investigated. The first failure occurred after 112 days of service. Replacement pipe failed 2 days later. Surface examination of the failed tubing indicated that fracture...
Series: ASM Handbook
Volume: 11
Publisher: ASM International
Published: 15 January 2021
DOI: 10.31399/asm.hb.v11.a0006772
EISBN: 978-1-62708-295-2
... examination Physical measurements Microscopic examination Light/stereomicroscopy Scanning electron microscopy Energy-dispersive spectroscopy Electrical measurements Radiography Computerized tomography Holography Liquid penetrant As previously noted, judgment calls often...
Series: ASM Handbook Archive
Volume: 11
Publisher: ASM International
Published: 01 January 2002
DOI: 10.31399/asm.hb.v11.a0003523
EISBN: 978-1-62708-180-1
... Physical measurements Microscopic examination Light/stereo microscopy Scanning electron microscopy Electrical measurements Radiography Holography Liquid penetrant As previously noted, judgement calls often have to be determined as to whether certain types of tests would...
Series: ASM Failure Analysis Case Histories
Volume: 3
Publisher: ASM International
Published: 01 December 2019
DOI: 10.31399/asm.fach.v03.c9001796
EISBN: 978-1-62708-241-9
... μm Fig. 7 Craters diameters on the outer raceway: histogram ( a ), classification ( b ). The average diameter of the craters measured 2.3 μm Despite the lack of a complete and definite model explaining all the processes that take place during electrical discharge, the best supported...
Series: ASM Failure Analysis Case Histories
Publisher: ASM International
Published: 01 June 2019
DOI: 10.31399/asm.fach.modes.c0046535
EISBN: 978-1-62708-234-1
..., three corrective measurements were implemented: The pipelines were asphalt coated The pipelines were enclosed in a concrete trough with a concrete cover Magnesium anodes, connected electrically to each line, were installed at periodic intervals along their entire length to provide cathodic...
Series: ASM Failure Analysis Case Histories
Publisher: ASM International
Published: 01 June 2019
DOI: 10.31399/asm.fach.aero.c0047076
EISBN: 978-1-62708-217-4
... not determine which. In other respects, the structure was normal in both areas. The condition of the plate was checked by hardness tests and by measurements of electrical conductivity. Hardness values ranged from 92 to 93 HRB. The electrical-conductivity values extended from 30.8 to 33.5% IACS ( Fig. 1a...
Series: ASM Failure Analysis Case Histories
Publisher: ASM International
Published: 01 June 2019
DOI: 10.31399/asm.fach.power.c9001594
EISBN: 978-1-62708-229-7
... Utilities Electric Company (TU Electric) has implemented in response to these failures. High-cycle fatigue is invisible to proven commercial nondestructive evaluation (NDE) methods during crack initiation and the initial phases of crack growth. Under a constant applied stress, cracks grow at accelerating...
Series: ASM Failure Analysis Case Histories
Publisher: ASM International
Published: 01 June 2019
DOI: 10.31399/asm.fach.matlhand.c9001453
EISBN: 978-1-62708-224-2
... to lift a casting weighing about 17 1 2 cwts. one of the links ruptured, causing injury to a workman. The sling, reputed to be of the electrically-welded steel type, was at least eight years old and had been overhauled several times during its working life. The links measured 2× 5 8...
Series: ASM Failure Analysis Case Histories
Publisher: ASM International
Published: 01 June 2019
DOI: 10.31399/asm.fach.mech.c0047939
EISBN: 978-1-62708-225-9
...Abstract Abstract Rough operation of the roller bearing mounted in an electric motor/gearbox assembly was observed. The bearing components made of low-alloy steel (4620 or 8620) and the cup, cone and rollers were carburized, hardened and tempered. The contact surfaces of these components (cup...
Series: ASM Handbook
Volume: 11
Publisher: ASM International
Published: 15 January 2021
DOI: 10.31399/asm.hb.v11.a0006764
EISBN: 978-1-62708-295-2
... difficult. Normally for qualitative comparison with reference sample. Part edges complicate results, and a skilled operator is required. No fluid coupling required. Can adapt to high-speed production lines Metals only Potential drop Measures electrical resistance between/among probes contacting...
Book Chapter

Series: ASM Handbook Archive
Volume: 11
Publisher: ASM International
Published: 01 January 2002
DOI: 10.31399/asm.hb.v11.a0003562
EISBN: 978-1-62708-180-1
.... , Unlubricated Fretting of Mild Steel in Air at Room Temperature, Part II: Electrical Contact Resistance Measurements and the Effect of Wear on Intermittent Loading , Wear , Vol 118 , 1987 , p 341 – 364 66. Iwabuchi A. , Kayaba T. , and Kata K. , Effect of Atmospheric Pressure...
Series: ASM Handbook Archive
Volume: 11
Publisher: ASM International
Published: 01 January 2002
DOI: 10.31399/asm.hb.v11.a0001810
EISBN: 978-1-62708-180-1
... measures to eliminate such stray currents include incorporation of insulation within bearing housings or at bearing pedestals and use of suitable short-circuiting connections between the rings or cones. Pitting of bearing elements by electrical action causes noisy bearing operation. In the following...
Series: ASM Handbook
Volume: 11A
Publisher: ASM International
Published: 30 August 2021
DOI: 10.31399/asm.hb.v11A.a0006834
EISBN: 978-1-62708-329-4
...Useful accuracy and clearance standards and how they can be measured Table 1 Useful accuracy and clearance standards and how they can be measured Structure type Rolling-element type Abbreviation Standard(s) Symbols, measuring tools, and techniques Radial Balls DGBB...
Series: ASM Failure Analysis Case Histories
Publisher: ASM International
Published: 01 June 2019
DOI: 10.31399/asm.fach.process.c9001443
EISBN: 978-1-62708-235-8
...Abstract Abstract Following the fusing of one of the copper leads in the choke circuit of an electric welder, a piece of the affected lead was obtained for examination. The sample had large internal cavities and surface bulges. It is remarkable that a wire containing defects of the magnitude...
Series: ASM Failure Analysis Case Histories
Volume: 1
Publisher: ASM International
Published: 01 December 1992
DOI: 10.31399/asm.fach.v01.c9001079
EISBN: 978-1-62708-214-3
... overboring of the rotor to remove indications close to the surface and revision of starting procedures, were implemented to extend the remaining life of the rotor and ensure its fitness for continued service. Cleavage Electric power generation Forgings Nonmetallic inclusions Cr-Mo-V Metalworking...
Series: ASM Failure Analysis Case Histories
Volume: 1
Publisher: ASM International
Published: 01 December 1992
DOI: 10.31399/asm.fach.v01.c9001120
EISBN: 978-1-62708-214-3
... at an electrical-discharge-machined surface where the resulting rehardened layer had not been removed. This rehardened layer had cracked, providing a source for fatigue initiation. Electrical discharge machining H13 UNS T20813 Fatigue fracture Metalworking-related failures Background Testing...
Series: ASM Failure Analysis Case Histories
Volume: 3
Publisher: ASM International
Published: 01 December 2019
DOI: 10.31399/asm.fach.v03.c9001827
EISBN: 978-1-62708-241-9
... effects of high-temperature oxidation on the hot corrosion process. Preventative measures are also discussed. gas turbine thermal fatigue cracking hot corrosion superalloys corrosion cavities spark optical emission spectrometry operating temperature GTD 111 (cast nickel-base superalloy) FSX...