Series: ASM Handbook
Volume: 11
Publisher: ASM International
Published: 15 January 2021
DOI: 10.31399/asm.hb.v11.a0006783
EISBN: 978-1-62708-295-2
... in binary alloys that contain phases of differing corrosion potentials. The grain in one phase becomes anodic to the grain in the second phase in the microstructure, thus producing an electrolytic cell when the proper electrolyte is present. Another illustration is ductile cast iron, where...
Book Chapter

Series: ASM Handbook Archive
Volume: 11
Publisher: ASM International
Published: 01 January 2002
DOI: 10.31399/asm.hb.v11.a0003548
EISBN: 978-1-62708-180-1
... illustrated in binary alloys that contain phases of differing corrosion potentials. The grain in one phase becomes anodic to grain in the second phase in the microstructure, thus producing an electrolytic cell when the proper electrolyte is present. Another illustration is ductile cast iron, where...