1-3 of 3 Search Results for

desiliconification

Follow your search
Access your saved searches in your account

Would you like to receive an alert when new items match your search?
Close Modal
Sort by
Series: ASM Failure Analysis Case Histories
Volume: 3
Publisher: ASM International
Published: 01 December 2019
DOI: 10.31399/asm.fach.v03.c9001772
EISBN: 978-1-62708-241-9
.... After a thorough examination, it was concluded that the part had failed due to dealloying via desiliconification. pump impeller corrosion erosion cast silicon bronze porosity microstructural analysis chemical composition Silicon bronze alloy UNS C86700 References 1...
Book Chapter

Series: ASM Handbook Archive
Volume: 11
Publisher: ASM International
Published: 01 January 2002
DOI: 10.31399/asm.hb.v11.a0003548
EISBN: 978-1-62708-180-1
... denickelification desiliconification dezincification galvanic corrosion graphitic corrosion intergranular corrosion pitting corrosion selective leaching uniform corrosion velocity-affected corrosion CORROSION is the electrochemical reaction of a material and its environment. This article addresses...
Series: ASM Handbook
Volume: 11
Publisher: ASM International
Published: 15 January 2021
DOI: 10.31399/asm.hb.v11.a0006783
EISBN: 978-1-62708-295-2