Series: ASM Handbook Archive
Volume: 11
Publisher: ASM International
Published: 01 January 2002
DOI: 10.31399/asm.hb.v11.a0003548
EISBN: 978-1-62708-180-1
... denickelification desiliconification dezincification galvanic corrosion graphitic corrosion intergranular corrosion pitting corrosion selective leaching uniform corrosion velocity-affected corrosion CORROSION is the electrochemical reaction of a material and its environment. This article addresses...
Series: ASM Failure Analysis Case Histories
Publisher: ASM International
Published: 01 June 2019
DOI: 10.31399/asm.fach.marine.c9001673
EISBN: 978-1-62708-227-3
..., selective dissolution of nickel (denickelification) from the alloy can also occur under special conditions, as outlined by Pickering and Wagner [ 5 ]. In the corrosion of cupronickels in seawater, the anodic process is dominated by: (Eq 1) Cu + 2 Cl − ⋅ ⇄ CuCl 2 − + e...
Series: ASM Handbook Archive
Volume: 11
Publisher: ASM International
Published: 01 January 2002
DOI: 10.31399/asm.hb.v11.a0001817
EISBN: 978-1-62708-180-1
... corrosion of copper alloys that leaves a spongy, structurally weak mass of the more noble alloying element in place at the site of corrosion attack. Selective leaching can occur in brasses (dezincification) and in copper-nickel alloys (denickelification). The net result of selective leaching is that sound...
Series: ASM Handbook
Volume: 11
Publisher: ASM International
Published: 15 January 2021
DOI: 10.31399/asm.hb.v11.a0006783
EISBN: 978-1-62708-295-2
Series: ASM Handbook
Volume: 11
Publisher: ASM International
Published: 15 January 2021
DOI: 10.31399/asm.hb.v11.a0006778
EISBN: 978-1-62708-295-2