1-20 of 55 Search Results for

control charts

Follow your search
Access your saved searches in your account

Would you like to receive an alert when new items match your search?
Close Modal
Sort by
Series: ASM Handbook Archive
Volume: 11
Publisher: ASM International
Published: 01 January 2002
DOI: 10.31399/asm.hb.v11.a0003519
EISBN: 978-1-62708-180-1
... funnel Plastic bags, 4 × 4 in. Sample collection Swabs Sample collection—always keep one for control sample Alloy reference list Materials, compositions, specifications, data Hardness Conversion Charts Martensitic and austenitic charts Addresses and phone numbers Assistance...
Series: ASM Handbook
Volume: 11
Publisher: ASM International
Published: 15 January 2021
DOI: 10.31399/asm.hb.v11.a0006755
EISBN: 978-1-62708-295-2
... during aircraft takeoffs and landings for many years. A bird may be ingested into an engine or strike the engine at takeoff or landing. The engine must be able to handle a bird strike without an uncontained failure, fire, or engine mount failure. An engine must be able to shut down in a controlled...
Series: ASM Failure Analysis Case Histories
Volume: 1
Publisher: ASM International
Published: 01 December 1992
DOI: 10.31399/asm.fach.v01.c9001093
EISBN: 978-1-62708-214-3
... following hot heading and prior to the production run. The process chart for hot heading was changed from water quenching to air cooling following the forming operation. Water quenching 8740 UNS G87400 Heat treating-related failures Intergranular fracture Background A heat-treated, cadmium...
Series: ASM Failure Analysis Case Histories
Publisher: ASM International
Published: 01 June 2019
DOI: 10.31399/asm.fach.aero.c9001587
EISBN: 978-1-62708-217-4
... of the jackscrew assembly, including the jackscrew with an internal torque tube, the gimbal nut, and the upper and lower mechanical stops. The jackscrew was connected to the horizontal stabilizer and controlled its movement. Multiple damage features, indicative of contact with another object, were observed...
Series: ASM Failure Analysis Case Histories
Publisher: ASM International
Published: 01 June 2019
DOI: 10.31399/asm.fach.machtools.c0047964
EISBN: 978-1-62708-223-5
... at each of the high points. The outside surface of the gear hub was a 3.8-cm (1 1 2 -in.) diam raceway for a radial-contact roller bearing. Examination of this surface disclosed a five-lobe contour having a 0.007-mm (0.00028-in.) (TIR) radial deviation. A chart trace on a rotary profile...
Series: ASM Handbook Archive
Volume: 11
Publisher: ASM International
Published: 01 January 2002
DOI: 10.31399/asm.hb.v11.a0003500
EISBN: 978-1-62708-180-1
..., design deficiencies, material defects, manufacturing/installation defects, and service life anomalies, with examples. The article describes several common charting methods that may be useful in performing an RCA. It also discusses other failure analysis tools, including review of all sources of input...
Series: ASM Handbook
Volume: 11
Publisher: ASM International
Published: 15 January 2021
DOI: 10.31399/asm.hb.v11.a0006753
EISBN: 978-1-62708-295-2
... on the processes involved in RCA and the charting methods that may be useful in RCA and ends with a description of various factors associated with failure prevention. corrosion distortion failure prevention fracture quality assurance root cause analysis wear MACHINES, COMPONENTS, and the materials...
Series: ASM Failure Analysis Case Histories
Publisher: ASM International
Published: 01 June 2019
DOI: 10.31399/asm.fach.process.c0048733
EISBN: 978-1-62708-235-8
..., the operators immediately went to the control room and found that the steam-temperature valve that admits steam to the brine heater was secured. However, the chart indicated that the brine temperature was 60 °C (140 °F) and that the pressure in the steam supply had increased. The steam valve was immediately...
Series: ASM Failure Analysis Case Histories
Volume: 2
Publisher: ASM International
Published: 01 December 1993
DOI: 10.31399/asm.fach.v02.c9001342
EISBN: 978-1-62708-215-0
.../Identification Corrosion or Wear Deposits EDXA analysis of the corrosion by-product from the outer bellows surface revealed significant peaks for chlorine and phosphorus ( Fig. 7 ). The strong chlorine peak indicated that the bellows failure was caused by chloride SCC. Fig. 7 EDXA chart...
Series: ASM Handbook Archive
Volume: 11
Publisher: ASM International
Published: 01 January 2002
DOI: 10.31399/asm.hb.v11.a0003521
EISBN: 978-1-62708-180-1
... with failures are present. These techniques are discussed in detail in the Section “Tools and Techniques in Failure Analysis” in this Volume. Damage mode identification chart Table 1 Damage mode identification chart Method Instantaneous failure mode (a) Progressive failure mode (b) Ductile...
Series: ASM Handbook
Volume: 11A
Publisher: ASM International
Published: 30 August 2021
DOI: 10.31399/asm.hb.v11A.a0006800
EISBN: 978-1-62708-329-4
...  Sound Walls, sound-absorbing wall surfaces Control motion Cams, grooves, slots, gears Allow passage (of light, rods, shafts, wires, pipes, etc.) Holes, windows, grooves Control or regulate the passage of:  Fluids Nozzles, orifices, pipes, ducts  Light Shutters, wheels Indicate...
Series: ASM Handbook
Volume: 11
Publisher: ASM International
Published: 15 January 2021
DOI: 10.31399/asm.hb.v11.a0006762
EISBN: 978-1-62708-295-2
... of the flow of the investigation and helps them understand the thought processes behind the analyses performed. Many experienced analysts prefer to put their conclusions at the beginning of a report, so the reader understands the pertinence of the information reported. Photographs, figures, charts, etc...
Series: ASM Handbook Archive
Volume: 11
Publisher: ASM International
Published: 01 January 2002
DOI: 10.31399/asm.hb.v11.a0003501
EISBN: 978-1-62708-180-1
...  Sound Walls, sound-absorbing wall surfaces Control motion Cams, grooves, slots, gears Allow passage (of light, rods, shafts, wires, pipes, etc.) Holes, windows, grooves Control or regulate the passage of  Fluids Nozzles, orifices, pipes, ducts  Light Shutters, wheels Indicate...
Series: ASM Failure Analysis Case Histories
Publisher: ASM International
Published: 01 June 2019
DOI: 10.31399/asm.fach.power.c9001609
EISBN: 978-1-62708-229-7
.... In the field, joints were wrapped with electrical resistance strip heaters and insulation. Temperature monitoring and control was by direct attachment of thermocouples and multiple channel controllers and chart recorders. The extra heat sink caused by the tube fins and the internal venting of heat due...
Series: ASM Failure Analysis Case Histories
Publisher: ASM International
Published: 01 June 2019
DOI: 10.31399/asm.fach.aero.c9001558
EISBN: 978-1-62708-217-4
... Abstract A liquid hydrogen main fuel control valve for a rocket engine failed by fracture of the Ti-5Al-2.5Sn body during the last of a series of static engine test firings. Fractographic, metallurgical, and stress analyses determined that a combination of fatigue and unexpected aqueous stress...
Series: ASM Handbook
Volume: 11A
Publisher: ASM International
Published: 30 August 2021
DOI: 10.31399/asm.hb.v11A.a0006817
EISBN: 978-1-62708-329-4
... specified interval Secondary functions Functions that a physical asset or system has to fulfill apart from its primary function(s), such as those needed to fulfill regulatory requirements and those that concern issues such as protection, control, containment, comfort, appearance, energy efficiency...
Series: ASM Handbook Archive
Volume: 11
Publisher: ASM International
Published: 01 January 2002
DOI: 10.31399/asm.hb.v11.a0003551
EISBN: 978-1-62708-180-1
... industry corrosion resistance gas turbine components heat exchangers material selection power generation industry process control refractories structural ceramics REFRACTORY MATERIALS are used in various industrial applications to line the interior of a multitude of vessels (mainly made...
Series: ASM Handbook Archive
Volume: 11
Publisher: ASM International
Published: 01 January 2002
DOI: 10.31399/asm.hb.v11.a0003534
EISBN: 978-1-62708-180-1
... of polymers (see the article “Characterization of Plastics in Failure Analysis” in this Volume). Table 2 is a summary chart of techniques discussed in this article. In this brief review, it is not possible to develop all the capabilities of each technique, but some of the more important attributes...
Series: ASM Handbook Archive
Volume: 11
Publisher: ASM International
Published: 01 January 2002
DOI: 10.31399/asm.hb.v11.a0003504
EISBN: 978-1-62708-180-1
... apart from its primary function(s), such as those needed to fulfill regulatory requirements and those that concern issues such as protection, control, containment, comfort, appearance, energy efficiency, and structural integrity User A person or organization that operates an asset or system and may...
Series: ASM Handbook
Volume: 11B
Publisher: ASM International
Published: 15 May 2022
DOI: 10.31399/asm.hb.v11B.a0006851
EISBN: 978-1-62708-395-9
..., and priority controls, such as aperture, shutter, and program. Additional features include capturing of multiple planes of focus with subsequent image stitching (Z-stacking) to produce full depth-of-field focus images. Some digital photography cameras also feature high-resolution video and audio recording...