EISBN: 978-1-62708-180-1
... in the environment; change in the alloy or heat treatment; change in design; use of galvanic protection; use of inhibitors; use of nonmetallic coatings and liners; application of metallic coatings; use of surface treatments, thermal spray, or other surface modifications; corrosion monitoring; and preventive...
Series: ASM Handbook
Volume: 11A
Publisher: ASM International
Published: 30 August 2021
DOI: 10.31399/asm.hb.v11A.a0006805
EISBN: 978-1-62708-329-4
... and uniformity of oxide coating. Etched with 2% nital. Original magnification: 1000× Fretting Fretting results from a very small movement of one highly loaded surface over another. The slight movement prevents the formation of, or destroys, any protective oxide film. Thus, continually clean surfaces...
Series: ASM Handbook Archive
Volume: 11
Publisher: ASM International
Published: 01 January 2002
DOI: 10.31399/asm.hb.v11.a0001812
EISBN: 978-1-62708-180-1
...-corrosion cracking, hydrogen embrittlement, and liquid-metal embrittlement of bolts and nuts. The article explains the most commonly used protective metal coatings for ferrous metal fasteners. Zinc, cadmium, and aluminum are commonly used for such coatings. The article also illustrates the performance...
Series: ASM Handbook
Volume: 11
Publisher: ASM International
Published: 15 January 2021
DOI: 10.31399/asm.hb.v11.a0006782
EISBN: 978-1-62708-295-2
... been dissolved. Iron is nearly inert in air-free water and seawater, because there is limited cathodic reaction possible. If the surface of the metal is coated with paint or other nonconducting film, the rates of both anodic and cathodic reactions are greatly reduced, and corrosion will be retarded...
Book Chapter

Series: ASM Handbook Archive
Volume: 11
Publisher: ASM International
Published: 01 January 2002
DOI: 10.31399/asm.hb.v11.a0003562
EISBN: 978-1-62708-180-1
...-resistant materials that are attached to the bone by means of screws of the same material. Fretting can occur between the underside of the screw head and the countersink of the hole in the plate. Fretting in this case results in disruption of otherwise protective films and the continual release of heavy...
Series: ASM Handbook
Volume: 11
Publisher: ASM International
Published: 15 January 2021
DOI: 10.31399/asm.hb.v11.a0006787
EISBN: 978-1-62708-295-2
... Abstract High-temperature corrosion can occur in numerous environments and is affected by various parameters such as temperature, alloy and protective coating compositions, stress, time, and gas composition. This article discusses the primary mechanisms of high-temperature corrosion, namely...
Series: ASM Handbook
Volume: 11
Publisher: ASM International
Published: 15 January 2021
DOI: 10.31399/asm.hb.v11.a0006829
EISBN: 978-1-62708-295-2
... fretting fatigue (i.e., crack nucleation and crack propagation) ( Ref 10 , 15 – 18 ). Fortunately, new surface treatments combining shot and laser peening with a thick self-lubricant plasma coating are now applied to prevent any critical damage process ( Ref 17 ). Fig. 3 Fretting wear damage...
Series: ASM Handbook
Volume: 11B
Publisher: ASM International
Published: 15 May 2022
DOI: 10.31399/asm.hb.v11B.a0006925
EISBN: 978-1-62708-395-9
... to produce waterborne systems and are cured by melamines. Solvent-based and waterborne container coatings are both used. In automotive applications, electrodeposited epoxides provide corrosion protection, and epoxy powder coatings are used in under-the-hood applications. Solid epoxies are used in pipe...