... lines are weaker than contiguous plastic surfaces and should be avoided, if possible, for high-impact products. This is why football helmets do not have ventilation holes, and auto bumpers are usually designed as contiguous uninterrupted surfaces. The gate was placed at the bezel center in Fig. 12...