1-7 of 7 Search Results for

cascade cleaning

Sort by
Series: ASM Failure Analysis Case Histories
Volume: 3
Publisher: ASM International
Published: 01 December 2019
DOI: 10.31399/asm.fach.v03.c9001841
EISBN: 978-1-62708-241-9
... to cleaning-induced damage concerns, many electronics industry cleaning procedures do not utilize ultrasound. These cleaning procedures include overflow and cascading rinse-baths, as well as spin and spray rinsing [ 5 ]. Any new cleaning process applied to small medical devices should be analyzed for each...
Series: ASM Handbook
Volume: 11
Publisher: ASM International
Published: 15 January 2021
DOI: 10.31399/asm.hb.v11.a0006771
EISBN: 978-1-62708-295-2
... characterization. Typical applications include identification of thin layers of contaminants on surfaces or at interfaces, evaluation of cleaning processes, corrosion studies, adhesion failures, and the identification of stains, oxides, and discolorations. Successful failure analysis can often be a matter...
Series: ASM Handbook Archive
Volume: 11
Publisher: ASM International
Published: 01 January 2002
DOI: 10.31399/asm.hb.v11.a0003534
EISBN: 978-1-62708-180-1
... or at interfaces, evaluation of cleaning processes, and the identification of stains and discolorations. Successful failure analysis can often be a matter of piecing together the different bits of information that different techniques can provide. Each of these three surface analysis techniques provides...
Series: ASM Handbook
Volume: 11B
Publisher: ASM International
Published: 15 May 2022
DOI: 10.31399/asm.hb.v11B.a0006943
EISBN: 978-1-62708-395-9
Series: ASM Handbook
Volume: 11
Publisher: ASM International
Published: 15 January 2021
DOI: 10.31399/asm.hb.v11.a0006764
EISBN: 978-1-62708-295-2
... attention to several concerns: Proper planning and sequencing of manufacturing methods and NDT procedures Avoidance of, or compensation for, adverse residual-stress effects Assurance of effective cleaning prior to processing with penetrant methods The balance of downtime and inspection costs...
Series: ASM Failure Analysis Case Histories
Publisher: ASM International
Published: 01 June 2019
DOI: 10.31399/asm.fach.design.c9001578
EISBN: 978-1-62708-233-4
... obtained for all the bearing locations on the pump train. The readings were at normal levels everywhere except in the horizontal direction on the high pressure (HP) pump. A level of 1.4 in./s was present at what appeared to be twice the running speed of the unit. A cascade plot of vibration on the HP pump...
Series: ASM Handbook
Volume: 11B
Publisher: ASM International
Published: 15 May 2022
DOI: 10.31399/asm.hb.v11B.9781627083959