Series: ASM Failure Analysis Case Histories
Publisher: ASM International
Published: 01 June 2019
DOI: 10.31399/asm.fach.design.c9001578
EISBN: 978-1-62708-233-4
... of the compressor. Reciprocating compressors have suction and discharge bottles to absorb the pressure pulsations from the pistons. This is similar to adding a capacitor to an electrical circuit to absorb the voltage ripple. Because the compressor unit was variable speed, the spectrum analyzer was set...