Image
Published: 01 June 2019
Fig. 6 Corrosion product build-up on a blue plastic header (a), degraded plastic and corroded Au bridgewire (b) after two years at 74 C. The corrosion produce on the solder is Au + In (OH) 2 Cl (c). The corroded bridgewire is shown in a stereo pair at the lower right (d). More
Series: ASM Handbook
Volume: 11A
Publisher: ASM International
Published: 30 August 2021
DOI: 10.31399/asm.hb.v11A.a0006838
EISBN: 978-1-62708-329-4
... be nested over and around each other in the build box. This ability to pack large batches of parts into a single build box makes for a very high-productivity printing scenario. Further, because postprocessing steps such as depowdering and sintering/infiltration can also be completed in large batches, binder...
Series: ASM Handbook
Volume: 11B
Publisher: ASM International
Published: 15 May 2022
DOI: 10.31399/asm.hb.v11B.a0006864
EISBN: 978-1-62708-395-9
... in the webline handling system Determine the critical draw ratio for the polymer: ○ Weakly non-Newtonian polymers: 20:1 ○ Strongly non-Newtonian polymers: 3:1 Reduce draw ratio Cool product faster so that it solidifies earlier Screw beat Improperly designed feed throat/screw Axial...
Series: ASM Handbook
Volume: 11B
Publisher: ASM International
Published: 15 May 2022
DOI: 10.31399/asm.hb.v11B.a0006914
EISBN: 978-1-62708-395-9
... – 507 5. Babich M. , Bevington C. , Chen X. , et al. , Project Plan: Organohalogen Flame Retardant Chemicals Assessment , Consumer Product Safety Commission , 2020 https://www.cpsc.gov/s3fs-public/OFR-plan-report-packagefinal.pdf?TDF6XKQhE3NgKpZaUZuTqVXXUW32E.kh Accessed...
Series: ASM Failure Analysis Case Histories
Publisher: ASM International
Published: 01 June 2019
DOI: 10.31399/asm.fach.bldgs.c9001701
EISBN: 978-1-62708-219-8
... not be based solely on product literature supplied by a manufacturer. Water treatment systems should be given strong consideration and implemented for use in all commercial buildings, residential complexes, and industrial facilities. Water treatment systems, if used should be continually monitored...
Series: ASM Failure Analysis Case Histories
Publisher: ASM International
Published: 01 June 2019
DOI: 10.31399/asm.fach.conag.c9001431
EISBN: 978-1-62708-221-1
... Abstract The sudden collapse of a tower crane on a building site resulted in severe injuries to the driver. Failure took place at the upper portion of the foundation or lowermost section. The mast sections were constructed from four main corner angles welded to end frames also made from angle...
Series: ASM Failure Analysis Case Histories
Volume: 1
Publisher: ASM International
Published: 01 December 1992
DOI: 10.31399/asm.fach.v01.c9001126
EISBN: 978-1-62708-214-3
... The spontaneous breakage of tempered glass spandrel panels used to cover concrete wall panels on building facades was investigated. Between January 1988 and August 1990, 19 panel failures were recorded. The tinted panels were coated on their exterior surfaces with a reflective metal oxide and covered on the back...
Series: ASM Failure Analysis Case Histories
Publisher: ASM International
Published: 01 June 2019
DOI: 10.31399/asm.fach.power.c9001700
EISBN: 978-1-62708-229-7
... solely on product literature supplied by a manufacturer. Water treatment systems should be given strong consideration and implemented for use in all commercial buildings, residential complexes, and industrial facilities. Water treatment systems, if used, should be continually monitored for signs...
Series: ASM Failure Analysis Case Histories
Publisher: ASM International
Published: 01 June 2019
DOI: 10.31399/asm.fach.usage.c9001430
EISBN: 978-1-62708-236-5
... involving both competence of welders subsequently employed on the job must also be assessed by carrying out the appropriate qualification tests. In many instances production tests plates may be called for and it is the usual practice for the item to be finally examined by non-destructive methods and a proof...
Series: ASM Failure Analysis Case Histories
Publisher: ASM International
Published: 01 June 2019
DOI: 10.31399/asm.fach.homegoods.c9001698
EISBN: 978-1-62708-222-8
... should not be based solely on product literature supplied by a manufacturer. Water treatment systems should be given strong consideration and implemented for use in all commercial buildings, residential complexes, and industrial facilities. Water treatment systems, if used should be continually...
Series: ASM Handbook
Volume: 11B
Publisher: ASM International
Published: 15 May 2022
DOI: 10.31399/asm.hb.v11B.a0006868
EISBN: 978-1-62708-395-9
... into production. Courtesy of Caroline MacLean-Blevins © 2017 Fig. 2 The plastic part development sequence includes creation of concepts, selection and validation of the concepts, and the detailed design and specification of the part. Fig. 3 Capture and document every functional requirement...
Series: ASM Failure Analysis Case Histories
Publisher: ASM International
Published: 01 June 2019
DOI: 10.31399/asm.fach.modes.c9001699
EISBN: 978-1-62708-234-1
... should not be based solely on product literature supplied by a manufacturer. Water treatment systems should be given strong consideration and implemented for use in all commercial buildings, residential complexes, and industrial facilities. Water treatment systems, if used, should be continually...
Series: ASM Handbook Archive
Volume: 11
Publisher: ASM International
Published: 01 January 2002
DOI: 10.31399/asm.hb.v11.a0003505
EISBN: 978-1-62708-180-1
... Abstract This article discusses the three legal theories on which a products liability lawsuit is based and the issues of hazard, risk, and danger in the context of liability. It describes manufacturing and design defects of various products. The article explains a design that is analyzed from...
Series: ASM Failure Analysis Case Histories
Publisher: ASM International
Published: 01 June 2019
DOI: 10.31399/asm.fach.conag.c9001432
EISBN: 978-1-62708-221-1
... the appropriate qualification tests. In many instances production tests plates may be called for and it is the usual practice for the item to be finally examined by non-destructive methods and a proof carried out. To the uninitiated on the other hand, welding appears on obviously simple process...
Series: ASM Failure Analysis Case Histories
Publisher: ASM International
Published: 01 June 2019
DOI: 10.31399/asm.fach.bldgs.c9001697
EISBN: 978-1-62708-219-8
... and materials selection on a project. Materials selection should not be based solely on product literature supplied by a manufacturer. Water treatment systems should be given strong consideration and implemented for use in all commercial buildings, residential complexes, and industrial facilities...
Series: ASM Failure Analysis Case Histories
Publisher: ASM International
Published: 01 June 2019
DOI: 10.31399/asm.fach.modes.c9001674
EISBN: 978-1-62708-234-1
... on a red plastic header. Fig. 6 Corrosion product build-up on a blue plastic header (a), degraded plastic and corroded Au bridgewire (b) after two years at 74 C. The corrosion produce on the solder is Au + In (OH) 2 Cl (c). The corroded bridgewire is shown in a stereo pair at the lower right (d...
Series: ASM Handbook
Volume: 11B
Publisher: ASM International
Published: 15 May 2022
DOI: 10.31399/asm.hb.v11B.a0006927
EISBN: 978-1-62708-395-9
... for the plastic forming processes covered. It also discusses the steps involved in design validation and verification. Reference Reference 1. MacLean-Blevins M.T. , Designing Successful Products with Plastics – Fundamentals of Plastic Part Design , first ed. , Elsevier , 2017 Selected...
Series: ASM Handbook
Volume: 11B
Publisher: ASM International
Published: 15 May 2022
DOI: 10.31399/asm.hb.v11B.9781627083959
EISBN: 978-1-62708-395-9
Series: ASM Handbook Archive
Volume: 11
Publisher: ASM International
Published: 01 January 2002
DOI: 10.31399/asm.hb.v11.a0003502
EISBN: 978-1-62708-180-1
... analyzing the design process that created the product, equipment, or system, as well as the physical failure itself. By using a systematic approach to the analysis, it is possible to review basic design issues and work toward the details in a progressive fashion. This helps to ensure that key points...
Series: ASM Failure Analysis Case Histories
Volume: 1
Publisher: ASM International
Published: 01 December 1992
DOI: 10.31399/asm.fach.v01.c9001094
EISBN: 978-1-62708-214-3
... the outer skin of a high-rise building. Fractographic and metallographic examination showed that the fractures occurred in a brittle manner from intergranular crack propagation. Laboratory and simulated environmental tests showed that an aqueous environment was necessary for the brittle fracture/cracking...