Series: ASM Failure Analysis Case Histories
Volume: 3
Publisher: ASM International
Published: 01 December 2019
DOI: 10.31399/asm.fach.v03.c9001785
EISBN: 978-1-62708-241-9
... that the failures stemmed from forging laps in the jaw that broaching failed to remove. open end wrench fracture forging laps chromium steel fracture scanning electron microscopy surface morphology chromium manganese steel (low alloy chromium steel, general) Introduction A maintenance worker...
Series: ASM Failure Analysis Case Histories
Volume: 3
Publisher: ASM International
Published: 01 December 2019
DOI: 10.31399/asm.fach.v03.c9001805
EISBN: 978-1-62708-241-9
... and whether or not the tool is meant to be re-used. As with most medical devices, there are tradeoffs for surgical tools between performance and expected lifetimes. For instance, the intended use condition for a hip implant broach handle involves striking the instrument with a hammer. In this case...
Series: ASM Handbook
Volume: 11A
Publisher: ASM International
Published: 30 August 2021
DOI: 10.31399/asm.hb.v11A.a0006826
EISBN: 978-1-62708-329-4
... acting as a reamer and the piston rod acting as a broach ( Ref 14 ). Unintentional irregularities or flaws ( Fig. 8 ) that occur at one place or at relatively infrequent or widely varying intervals on the surface are often not detected and included in roughness measurements. Flaws such as cracks...
Series: ASM Handbook
Volume: 11A
Publisher: ASM International
Published: 30 August 2021
DOI: 10.31399/asm.hb.v11A.9781627083294
EISBN: 978-1-62708-329-4