... in the ingot can seriously affect the quality and performance of wrought products. The major ingot imperfections are: Chemical segregation Ingot pipe, porosity, and centerline shrinkage High hydrogen content Nonmetallic inclusions Unmelted electrodes and shelf Cracks, laminations, seams...
Series: ASM Failure Analysis Case Histories
Volume: 3
Publisher: ASM International
Published: 01 December 2019
DOI: 10.31399/asm.fach.v03.c9001803
EISBN: 978-1-62708-241-9
.... , Buckley C.A. , et al. : “ Intergranular Corrosion-Fatigue Failure of Cobalt-Alloy Femoral Stems ,” J. Bone Joint Surg. Am. , 1994 , 76 ( 1 ), pp. 110 – 115 10.2106/00004623-199401000-00014 . 15. Chaodi L. , Christopher G. , et al. : “ Progressive Failure Analysis of Laminated...
Series: ASM Handbook Archive
Volume: 11
Publisher: ASM International
Published: 01 January 2002
DOI: 10.31399/asm.hb.v11.a0003507
EISBN: 978-1-62708-180-1
.... The article discusses the types of imperfections that can be traced to the original ingot product. These include chemical segregation; ingot pipe, porosity, and centerline shrinkage; high hydrogen content; nonmetallic inclusions; unmelted electrodes and shelf; and cracks, laminations, seams, pits, blisters...
Series: ASM Handbook
Volume: 11
Publisher: ASM International
Published: 15 January 2021
DOI: 10.31399/asm.hb.v11.9781627082952
EISBN: 978-1-62708-295-2
Series: ASM Handbook
Volume: 11A
Publisher: ASM International
Published: 30 August 2021
DOI: 10.31399/asm.hb.v11A.a0006838
EISBN: 978-1-62708-329-4
... Directed-energy deposition Material extrusion Binder jetting Sheet lamination Since approximately 2010, AM technology has transitioned from a relatively obscure collection of processes into an important engineering tool with active engineering developments ( Ref 3 – 5 ) for a wide range...
Series: ASM Handbook Archive
Volume: 11
Publisher: ASM International
Published: 01 January 2002
DOI: 10.31399/asm.hb.v11.a0003524
EISBN: 978-1-62708-180-1
... to isolate the variables. In some instances, ultrasonic testing has proved to be a useful tool in failure analysis, particularly in the investigation of large castings and forgings. Cracks, laminations, shrinkage cavities, bursts, flakes, pores, disbonds, and other discontinuities that produce reflective...
Series: ASM Handbook Archive
Volume: 11
Publisher: ASM International
Published: 01 January 2002
DOI: 10.31399/asm.hb.v11.a0003537
EISBN: 978-1-62708-180-1
... at that location because no normal stress acts at the centerline. (There is a shear stress at this location in bending, but in a homogeneous material, it is too small to initiate fracture. That might not be the case for a laminated structure loaded in bending.) Alternatively, brittle torsion failure is readily...
Series: ASM Handbook
Volume: 11
Publisher: ASM International
Published: 15 January 2021
DOI: 10.31399/asm.hb.v11.a0006774
EISBN: 978-1-62708-295-2
Series: ASM Handbook
Volume: 11A
Publisher: ASM International
Published: 30 August 2021
DOI: 10.31399/asm.hb.v11A.9781627083294
EISBN: 978-1-62708-329-4
Series: ASM Handbook
Volume: 11A
Publisher: ASM International
Published: 30 August 2021
DOI: 10.31399/asm.hb.v11A.a0006812
EISBN: 978-1-62708-329-4
... misalignment and shell distortion Cracklike flaws Creep damage Fire damage assessment Dents and gouges Laminations First published in 2000 as an API recommended practice (API RP 579), its 2007 second edition was published as an API standard/American Society of Mechanical Engineers (ASME...