1-20 of 131 Search Results for

aluminum-based casting alloys

Follow your search
Access your saved searches in your account

Would you like to receive an alert when new items match your search?
Close Modal
Sort by
Series: ASM Handbook
Volume: 11A
Publisher: ASM International
Published: 30 August 2021
DOI: 10.31399/asm.hb.v11A.a0006831
EISBN: 978-1-62708-329-4
... for potential casting applications so that the likelihood of failure to perform the intended function is decreased. The article addresses factors that may cause failures in castings for each metal type, starting with gray iron and progressing to ductile iron, steel, aluminum, and copper-base alloys...
Series: ASM Failure Analysis Case Histories
Publisher: ASM International
Published: 01 June 2019
DOI: 10.31399/asm.fach.process.c9001522
EISBN: 978-1-62708-235-8
...Abstract Abstract In the EMD-2 Joint Directed Attack Munition (JDAM), the A357 aluminum alloy housing had been redesigned and cast via permanent mold casting, but did not meet the design strength requirements of the previous design. Mechanical tests on thick and thin sections of the forward...
Series: ASM Failure Analysis Case Histories
Volume: 1
Publisher: ASM International
Published: 01 December 1992
DOI: 10.31399/asm.fach.v01.c9001082
EISBN: 978-1-62708-214-3
... impellers made of nickel-aluminum-bronze, newly cast type 304L stainless steel pump impellers were installed. Type 304L stainless steel was chosen because its erosion-resistant properties were superior to those of nickel-aluminum-bronze alloy. The plant owners, rather than the pump manufacturers, changed...
Book Chapter

Series: ASM Handbook Archive
Volume: 11
Publisher: ASM International
Published: 01 January 2002
DOI: 10.31399/asm.hb.v11.a0003548
EISBN: 978-1-62708-180-1
... damaging, although not fully compatible with magnesium. Aluminum alloys containing small percentages of copper (7000 and 2000 series and 380 die-casting alloy) may cause serious galvanic corrosion of magnesium in saline environments. Very pure aluminum is quite compatible, acting as a polarizable...
Series: ASM Handbook Archive
Volume: 11
Publisher: ASM International
Published: 01 January 2002
DOI: 10.31399/asm.hb.v11.a0003508
EISBN: 978-1-62708-180-1
... casting. Cast iron, gray cast iron, malleable irons, ductile iron, low-alloy steel castings, austenitic steels, corrosion-resistant castings, and cast aluminum alloys are the materials discussed. The article describes the general types of discontinuities or imperfections for traditional casting with sand...
Series: ASM Handbook Archive
Volume: 11
Publisher: ASM International
Published: 01 January 2002
DOI: 10.31399/asm.hb.v11.a0003529
EISBN: 978-1-62708-180-1
... of information, in particular, when the analyst is not very familiar with the alloy system in question. For example, the potential consequences of exceeding impurity limits for zinc and aluminum casting alloys are discussed in various articles in Properties and Selection: Nonferrous Alloys and Special...
Series: ASM Failure Analysis Case Histories
Volume: 3
Publisher: ASM International
Published: 01 December 2019
DOI: 10.31399/asm.fach.v03.c9001781
EISBN: 978-1-62708-241-9
...% of the composition are listed in Table 1 . Based on the subject and exemplar golf club hosels’ elemental composition, the material closely resembles A360 cast aluminum. The composition of A360.0 cast aluminum alloy [ 15 ] for comparison is listed in Table 1 as well. From the compression test data, the stress...
Series: ASM Failure Analysis Case Histories
Volume: 1
Publisher: ASM International
Published: 01 December 1992
DOI: 10.31399/asm.fach.v01.c9001029
EISBN: 978-1-62708-214-3
...Abstract Abstract Two investment-cast A356 aluminum alloy actuators used for handles on passenger doors of commercial aircraft fractured during torquing at less than the design load. Visual examination showed that cracking had occurred through a machined side hole. Fractography revealed...
Series: ASM Handbook
Volume: 11A
Publisher: ASM International
Published: 30 August 2021
DOI: 10.31399/asm.hb.v11A.9781627083294
EISBN: 978-1-62708-329-4
Series: ASM Handbook
Volume: 11
Publisher: ASM International
Published: 15 January 2021
DOI: 10.31399/asm.hb.v11.a0006783
EISBN: 978-1-62708-295-2
... to galvanic corrosion. Metals that combine active potentials with higher hydrogen overvoltages, such as aluminum, zinc, cadmium, and tin, are much less damaging, although not fully compatible with magnesium. Aluminum alloys that contain small percentages of copper (7000 and 2000 series and 380 die-casting...
Series: ASM Failure Analysis Case Histories
Volume: 3
Publisher: ASM International
Published: 01 December 2019
DOI: 10.31399/asm.fach.v03.c9001760
EISBN: 978-1-62708-241-9
... be prevented by eliminating the bolt hole, using a different type of bolt, or adjusting the fastening torque. cylinder head overload failure overtorquing cast aluminum alloy casting pores metallurgical analysis thermomechanical fatigue strength EN 46200 (aluminum alloy AlSi8Cu3) Introduction...
Series: ASM Handbook
Volume: 11
Publisher: ASM International
Published: 15 January 2021
DOI: 10.31399/asm.hb.v11.a0006778
EISBN: 978-1-62708-295-2
... ( Fig. 1a , b ). Parabolic or elongated shear dimples occur from torsional loading ( Fig. 1c ) or from mode II (in-plane) shear. However, metallic materials can behave in a ductile manner but not exhibit the classical dimple-rupture morphology, as shown in Fig. 1(d) for a cast aluminum alloy...
Series: ASM Handbook Archive
Volume: 11
Publisher: ASM International
Published: 01 January 2002
DOI: 10.31399/asm.hb.v11.a0003536
EISBN: 978-1-62708-180-1
... length through Si particles was observed to be 0.16 in the vertical section fracture profile of a tensile fracture surface of chill cast A356 aluminum alloy having a volume fraction of Si particle equal to 0.074. In this case, as P f is significantly higher than the silicon particle volume fraction...
Series: ASM Failure Analysis Case Histories
Volume: 3
Publisher: ASM International
Published: 01 December 2019
DOI: 10.31399/asm.fach.v03.c9001753
EISBN: 978-1-62708-241-9
.... The chemical composition of the sand-cast component was identified via optical emission spectroscopy and is comparable to an aluminum sand-cast alloy, AA 712.0. Metallographic evaluation via optical microscopy and scanning electron microscopy revealed a high degree of porosity in the microstructure as well...
Series: ASM Failure Analysis Case Histories
Publisher: ASM International
Published: 01 June 2019
DOI: 10.31399/asm.fach.usage.c0046366
EISBN: 978-1-62708-236-5
...Abstract Abstract Several large chromium-plated 4340 steel cylinders were removed from service because of deep longitudinal score marks in the plating. One of the damaged cylinders and a mating cast aluminum alloy B850-T5 bearing adapter that also exhibited deep longitudinal score marks were...
Series: ASM Failure Analysis Case Histories
Publisher: ASM International
Published: 01 June 2019
DOI: 10.31399/asm.fach.process.c9001908
EISBN: 978-1-62708-235-8
... Valentin Frunza and Dennis Klaszewski of NAWCWD for their editorial and technical contributions. ARL conducted an analysis of two semicircular aluminum die-castings (Alloy A356) that are components of the tailcone assembly of the Rockeye Cluster Bomb. As the name implies, these components are located...
Series: ASM Failure Analysis Case Histories
Publisher: ASM International
Published: 01 June 2019
DOI: 10.31399/asm.fach.auto.c9001543
EISBN: 978-1-62708-218-1
..., virtually all such pistons are cast aluminum. The preferred alloy is 357 aluminum, which contains 6.5 to 7.5 Si and 0.45 to 0.60 Mg. Tensile strength is 45,000 to 52,000 psi in solution treated, aged stock. Forged pistons are also used, but the gain in mechanical properties comes at a higher cost...
Series: ASM Handbook Archive
Volume: 11
Publisher: ASM International
Published: 01 January 2002
DOI: 10.31399/asm.hb.v11.a0003543
EISBN: 978-1-62708-180-1
... manner, but not exhibit the classical dimple-rupture morphology, as shown in Fig. 1(d) for a cast aluminum alloy. The cast aluminum alloy fracture surface should show dimples in the aluminum matrix (original dendrites), but can be difficult to see because fracture surface morphology is impacted...
Series: ASM Failure Analysis Case Histories
Publisher: ASM International
Published: 01 June 2019
DOI: 10.31399/asm.fach.petrol.c9001638
EISBN: 978-1-62708-228-0
... of the oxide forming elements near the alloy surface interferes with the process of formation of the protective scale. If sufficient sulfur enters the alloy and all immediately available chromium or aluminum is converted to sulfides, then the less stable sulfides of the base metal may form. 6 Under...
Series: ASM Failure Analysis Case Histories
Publisher: ASM International
Published: 01 June 2019
DOI: 10.31399/asm.fach.process.c9001640
EISBN: 978-1-62708-235-8
... by the presence of surface imperfections. Improving the surface finish or choosing a stronger alloy, were more likely to improve part durability than reducing the porosity. Complex failures Data interpretation Deviations from ideality Thinking errors Aluminum casting Casting-related failures A new...