1-20 of 261 Search Results for

agriculture equipment

Follow your search
Access your saved searches in your account

Would you like to receive an alert when new items match your search?
Close Modal
Sort by
Series: ASM Failure Analysis Case Histories
Publisher: ASM International
Published: 01 June 2019
DOI: 10.31399/asm.fach.conag.9781627082211
EISBN: 978-1-62708-221-1
Series: ASM Failure Analysis Case Histories
Volume: 1
Publisher: ASM International
Published: 01 December 1992
DOI: 10.31399/asm.fach.v01.c9001039
EISBN: 978-1-62708-214-3
... that bridged a wide gap. The most probable cause of failure was improper preheat during welding. Agricultural equipment Fillet welds 4140 UNS G41400 Joining-related failures Fatigue fracture Background The 4140 steel steering spindle on a tricycle agricultural field chemical applicator...
Series: ASM Failure Analysis Case Histories
Publisher: ASM International
Published: 01 June 2019
DOI: 10.31399/asm.fach.conag.c0051294
EISBN: 978-1-62708-221-1
... Abstract An agricultural tine, which is a relatively large double torsion spring with outer legs that are used to sweep through hay or other crops and turn them over, had failed. It was made hard-drawn carbon steel. Bending fatigue was revealed by visual examination to be almost certainly...
Series: ASM Failure Analysis Case Histories
Publisher: ASM International
Published: 01 June 2019
DOI: 10.31399/asm.fach.conag.c9001500
EISBN: 978-1-62708-221-1
... diagonally across the profile of the loaded side, which was consistent on every tooth. Agricultural equipment Bevel gears Design Loads (forces) Tractors 4820H UNS H48200 Rolling-contact wear Fatigue fracture A spiral bevel gear and pinion set was submitted for examination and evaluation...
Series: ASM Failure Analysis Case Histories
Publisher: ASM International
Published: 01 June 2019
DOI: 10.31399/asm.fach.conag.c0045987
EISBN: 978-1-62708-221-1
Series: ASM Failure Analysis Case Histories
Publisher: ASM International
Published: 01 June 2019
DOI: 10.31399/asm.fach.conag.c9001464
EISBN: 978-1-62708-221-1
Series: ASM Failure Analysis Case Histories
Publisher: ASM International
Published: 01 June 2019
DOI: 10.31399/asm.fach.conag.c0048082
EISBN: 978-1-62708-221-1
Series: ASM Failure Analysis Case Histories
Publisher: ASM International
Published: 01 June 2019
DOI: 10.31399/asm.fach.conag.c9001414
EISBN: 978-1-62708-221-1
Series: ASM Failure Analysis Case Histories
Publisher: ASM International
Published: 01 June 2019
DOI: 10.31399/asm.fach.conag.c0047474
EISBN: 978-1-62708-221-1
.... , Failures of Lifting Equipment , Failure Analysis and Prevention , Vol 11 , ASM Handbook , ASM International , 1986 , p 514 – 528 10.31399/asm.hb.v11.a0001811 • Failures Related to Casting , Failure Analysis and Prevention , Vol 11 , ASM Handbook , ASM International , 2002 , p 103 – 155...
Series: ASM Failure Analysis Case Histories
Publisher: ASM International
Published: 01 June 2019
DOI: 10.31399/asm.fach.conag.c9001466
EISBN: 978-1-62708-221-1
... Selected References • Jamieson F.L. , Failures of Lifting Equipment , Failure Analysis and Prevention , Vol 11 , ASM Handbook , ASM International , 1986 , p 514 – 528 10.31399/asm.hb.v11.a0001811 • Fatigue Failures , Failure Analysis and Prevention , Vol 11 , ASM Handbook...
Series: ASM Failure Analysis Case Histories
Publisher: ASM International
Published: 01 June 2019
DOI: 10.31399/asm.fach.conag.c0090938
EISBN: 978-1-62708-221-1
Series: ASM Failure Analysis Case Histories
Publisher: ASM International
Published: 01 June 2019
DOI: 10.31399/asm.fach.conag.c0048077
EISBN: 978-1-62708-221-1
Series: ASM Failure Analysis Case Histories
Publisher: ASM International
Published: 01 June 2019
DOI: 10.31399/asm.fach.conag.c9001248
EISBN: 978-1-62708-221-1
Series: ASM Failure Analysis Case Histories
Publisher: ASM International
Published: 01 June 2019
DOI: 10.31399/asm.fach.conag.c0047479
EISBN: 978-1-62708-221-1
Series: ASM Failure Analysis Case Histories
Publisher: ASM International
Published: 01 June 2019
DOI: 10.31399/asm.fach.conag.c0047212
EISBN: 978-1-62708-221-1
... to fracture. No evidence of a defective design, improper microstructure, high inclusion count, or other stress-raising condition was observed. No recommendations were made. Earthmoving equipment Plastic deformation Shafts (power) 4340 UNS G43400 Fatigue fracture A steering knuckle used...
Series: ASM Failure Analysis Case Histories
Publisher: ASM International
Published: 01 June 2019
DOI: 10.31399/asm.fach.conag.c9001495
EISBN: 978-1-62708-221-1
... and should have withstood normal operating conditions. The spacing of the gouge marks coincided with the spacing of the splines, indicative of careless assembly with the mating wheel gear. Assembling Axles Mining equipment Splines 4340 UNS G43400 Fatigue fracture One end of a broken axle...
Series: ASM Failure Analysis Case Histories
Publisher: ASM International
Published: 01 June 2019
DOI: 10.31399/asm.fach.conag.c9001468
EISBN: 978-1-62708-221-1
... possible and the likelihood of serious accidents removed. Selected References Selected References • Jamieson F.L. , Failures of Lifting Equipment , Failure Analysis and Prevention , Vol 11 , ASM Handbook , ASM International , 1986 , p 514 – 528 10.31399/asm.hb.v11.a0001811...
Book Chapter

Series: ASM Failure Analysis Case Histories
Publisher: ASM International
Published: 01 June 2019
DOI: 10.31399/asm.fach.conag.c9001419
EISBN: 978-1-62708-221-1
... occurred under the excessively severe torsional stresses introduced when the emergency brake was applied. Selected References Selected References • Jamieson F.L. , Failures of Lifting Equipment , Failure Analysis and Prevention , Vol 11 , ASM Handbook , ASM International , 1986 , p...
Series: ASM Failure Analysis Case Histories
Volume: 2
Publisher: ASM International
Published: 01 December 1993
DOI: 10.31399/asm.fach.v02.c9001386
EISBN: 978-1-62708-215-0
.... Prevention of such corrosion by the use of a flexible sealant to eliminate the crevice was recommended. Agricultural equipment Bolted joints Brittle fracture Pressure cells Stress-corrosion cracking 420 UNS S42000 Pitting corrosion Corrosion fatigue Fatigue fracture Background Two type...
Series: ASM Failure Analysis Case Histories
Publisher: ASM International
Published: 01 June 2019
DOI: 10.31399/asm.fach.conag.c0047508
EISBN: 978-1-62708-221-1