1-20 of 22 Search Results for

aerospace and military applications

Follow your search
Access your saved searches in your account

Would you like to receive an alert when new items match your search?
Close Modal
Sort by
Series: ASM Failure Analysis Case Histories
Volume: 1
Publisher: ASM International
Published: 01 December 1992
DOI: 10.31399/asm.fach.v01.c9001030
EISBN: 978-1-62708-214-3
...). Control of machining parameters to prevent formation of brittle martensite, use of galvanically compatible fasteners, and use of an alternate lubricant were recommended. Airframes, corrosion Fasteners Jet planes Marine environments Military planes Solid lubricants Ti-6Al-4V UNS R56406 Stress...
Series: ASM Handbook Archive
Volume: 11
Publisher: ASM International
Published: 01 January 2002
DOI: 10.31399/asm.hb.v11.a0003515
EISBN: 978-1-62708-180-1
...-inspection defect distributions shown in Fig. 6 . As an example, consider the application of damage tolerance to military aircraft engines ( Ref 16 ), a part of the USAF Engine Structural Integrity Program (ENSIP). In this example, components are designed for crack growth so that the safety limit...
Series: ASM Failure Analysis Case Histories
Volume: 1
Publisher: ASM International
Published: 01 December 1992
DOI: 10.31399/asm.fach.v01.c9001023
EISBN: 978-1-62708-214-3
.... The wear had been caused by incorrect machining of the shaft splines, which prevented the bevel gear nut from locating correctly against the gear. Aerospace engines Aircraft components Bevel gears Drives Engine components Jet planes Military planes Splines 16 NCD 13 Fretting wear...
Series: ASM Failure Analysis Case Histories
Publisher: ASM International
Published: 01 June 2019
DOI: 10.31399/asm.fach.aero.c9001706
EISBN: 978-1-62708-217-4
... , ( 1990 ) 6. Military Specification MIL-C-16173E , Corrosion Preventive Compounds-Solvent Cutback Cold Application, (1993) 7. Military Handbook 5F , Metallic Materials & Elements for Aerospace Vehicle structures, Vol.1 , pp 2 –31 to 2– 51 ( 1990 ) Selected References Selected...
Series: ASM Handbook Archive
Volume: 11
Publisher: ASM International
Published: 01 January 2002
DOI: 10.31399/asm.hb.v11.a0003503
EISBN: 978-1-62708-180-1
... in terms of their consequences. During the 1970s and '80s, various military and professional society standards were written to define the analysis methodology ( Ref 5 , 6 , 7 , 8 ). MIL-STD 1629 (ships), “Procedures For Performing a Failure Mode Effects and Criticality Analysis” ( Ref 9 ) was published...
Series: ASM Failure Analysis Case Histories
Volume: 1
Publisher: ASM International
Published: 01 December 1992
DOI: 10.31399/asm.fach.v01.c9001081
EISBN: 978-1-62708-214-3
... Abstract Several compressor disks in military fighter and trainer aircraft gas turbine engines cracked prematurely in the bolt hole regions. The disks were made of precipitation-hardened AM355 martensitic stainless steel. Experimental and analytical work was performed on specimens from...
Series: ASM Handbook
Volume: 11A
Publisher: ASM International
Published: 30 August 2021
DOI: 10.31399/asm.hb.v11A.a0006805
EISBN: 978-1-62708-329-4
... cost of a fastener failure. Adequate testing is the most practical method of guarding against failure of a new fastener system for a critical application. The designer must not extrapolate existing data to a different size of the same fastener, because larger-diameter fasteners have significantly lower...
Series: ASM Handbook Archive
Volume: 11
Publisher: ASM International
Published: 01 January 2002
DOI: 10.31399/asm.hb.v11.a0001812
EISBN: 978-1-62708-180-1
... of specification and qualification controls. The extent and complexity of the system needed is usually dictated by the probable cost of a fastener failure. Adequate testing is the most practical method of guarding against failure of a new fastener system for a critical application. The designer must...
Series: ASM Handbook Archive
Volume: 11
Publisher: ASM International
Published: 01 January 2002
DOI: 10.31399/asm.hb.v11.a0003516
EISBN: 978-1-62708-180-1
.... The article concludes with case studies of fatigue life assessment from the aerospace industry. aerospace industry aluminum crack growth software damage-tolerance approach fatigue crack growth fatigue-life assessment fracture mechanics retardation spectrum load steel stress spectrum stress...
Series: ASM Handbook
Volume: 11A
Publisher: ASM International
Published: 30 August 2021
DOI: 10.31399/asm.hb.v11A.a0006819
EISBN: 978-1-62708-329-4
... components, equipment, and structures has long been a serious safety and reliability concern for countless manufacturing, construction, and transportation industries, including automotive, aerospace, marine, power generation, chemical processing, and oil and gas. Furthermore, fatigue failures have been...
Series: ASM Handbook
Volume: 11
Publisher: ASM International
Published: 15 January 2021
DOI: 10.31399/asm.hb.v11.a0006753
EISBN: 978-1-62708-295-2
... A concise problem-solving model, adapted from several of the referenced authors, and that has specific applicability to this Volume, is depicted in Fig. 2 . The continuous, circular format in the graphic is significant, indicating that the process reinitiates with the identification of a new problem...
Series: ASM Handbook
Volume: 11
Publisher: ASM International
Published: 15 January 2021
DOI: 10.31399/asm.hb.v11.a0006759
EISBN: 978-1-62708-295-2
... in the United States for engineered metals are International Organization for Standardization (ISO), American Society for Testing and Materials (ASTM), Society of Automotive Engineers (SAE), Aerospace Materials Specifications (AMS), American Iron and Steel Institute (AISI), and military standards (MIL), which...
Series: ASM Handbook Archive
Volume: 11
Publisher: ASM International
Published: 01 January 2002
DOI: 10.31399/asm.hb.v11.a0003556
EISBN: 978-1-62708-180-1
..., drinking water supply, pulp and paper making, and other industrial sectors. Microbially induced corrosion is also a concern whenever metals are exposed directly to the environment in applications including marine or buried piping, storage tanks, ships, nuclear waste containers, pilings, marine platforms...
Series: ASM Handbook Archive
Volume: 11
Publisher: ASM International
Published: 01 January 2002
DOI: 10.31399/asm.hb.v11.a0003512
EISBN: 978-1-62708-180-1
... and therefore when “failure” occurs. Defining failure is also related to what is meant by the “design life.” For example, for the aerospace industry, an airplane may be designed for 8000 flight hours and analyzed for two lifetimes or 16,000 flight hours. For the power industry, the design life of components...
Series: ASM Handbook
Volume: 11A
Publisher: ASM International
Published: 30 August 2021
DOI: 10.31399/asm.hb.v11A.a0006802
EISBN: 978-1-62708-329-4
..., for the aerospace industry, an airplane may be designed for 8000 flight hours and analyzed for two lifetimes or 16,000 flight hours. For the power industry, the design life of components is sometimes taken as 40 years. This means that the equipment is expected to perform satisfactorily at its rated output for 40...
Series: ASM Handbook
Volume: 11A
Publisher: ASM International
Published: 30 August 2021
DOI: 10.31399/asm.hb.v11A.a0006831
EISBN: 978-1-62708-329-4
... Abstract The information provided in this article is intended for those individuals who want to determine why a casting component failed to perform its intended purpose. It is also intended to provide insights for potential casting applications so that the likelihood of failure to perform...
Series: ASM Handbook
Volume: 11A
Publisher: ASM International
Published: 30 August 2021
DOI: 10.31399/asm.hb.v11A.9781627083294
EISBN: 978-1-62708-329-4
Series: ASM Handbook
Volume: 11B
Publisher: ASM International
Published: 15 May 2022
DOI: 10.31399/asm.hb.v11B.9781627083959
EISBN: 978-1-62708-395-9
Series: ASM Handbook Archive
Volume: 11
Publisher: ASM International
Published: 01 January 2002
DOI: 10.31399/asm.hb.v11.a0003524
EISBN: 978-1-62708-180-1
... application, or related to the material properties, design, or manufacture of the product. In cases that involve personal injury or will most likely involve legal pursuit of compensation from another company, care must be taken in preserving the scene and physical evidence. Accidental or deliberate...
Series: ASM Handbook
Volume: 11
Publisher: ASM International
Published: 15 January 2021
DOI: 10.31399/asm.hb.v11.a0006787
EISBN: 978-1-62708-295-2
... Further graphite deposition from the gas phase on the catalytically active metal particles (iron, nickel) For example, chemical reactions producing such high carbon activities in reformer applications are: (Eq 1) Hydrogen reformer : CH 4 + H 2 O ↔ CO + 3H 2...