Series: ASM Failure Analysis Case Histories
Volume: 2
Publisher: ASM International
Published: 01 December 1993
DOI: 10.31399/asm.fach.v02.c9001749
EISBN: 978-1-62708-215-0
...Abstract Abstract An oxygen line that was part of a mobile, truck -mounted oxygen-acetylene welding unit exploded in service. Analysis revealed that the failure occurred at the flexible hose-to-valve connection. It was further determined that a steel adapter had been installed at the point...
Series: ASM Failure Analysis Case Histories
Publisher: ASM International
Published: 01 June 2019
DOI: 10.31399/asm.fach.process.c9001447
EISBN: 978-1-62708-235-8
... the electrical conductivity and a small amount of oxygen is unavoidable in materials for conductors in electrical engineering. In gas welding even a neutral oxygen-acetylene flame will cause “gassing” as seen in Figure 11 . Although the use of a shielding gas will serve to prevent this to a large extent...
Series: ASM Failure Analysis Case Histories
Publisher: ASM International
Published: 01 June 2019
DOI: 10.31399/asm.fach.homegoods.c9001677
EISBN: 978-1-62708-222-8
... continuous load application until fracture occurred. A fourth strip was fatigued by bending the strip back and forth until fracture occurred. A fifth strip was heated with an oxy-acetylene torch while the material was twisted to fracture. The results from these tests were then compared with the original...