Series: ASM Failure Analysis Case Histories
Volume: 1
Publisher: ASM International
Published: 01 December 1992
DOI: 10.31399/asm.fach.v01.c9001123
EISBN: 978-1-62708-214-3
...Abstract Abstract Extensive cracking was found in a batch of die-cast ZAMAK 3 solenoid valve seats during commissioning of the system in which they were installed. Scanning electron microscopic and chemical analyses conducted on one of the failed valve seats showed that the composition...