Series: ASM Failure Analysis Case Histories
Publisher: ASM International
Published: 01 June 2019
DOI: 10.31399/asm.fach.design.c0091358
EISBN: 978-1-62708-233-4
... Abstract After about two years in service, a 303 stainless steel valve in contact with a carbonated soft drink in a vending machine occasionally dispensed a discolored drink with a sulfide odor. According to the laboratory at the bottling plant, the soft drink in question was strongly acidic...
Image
Published: 01 January 2002
Fig. 33 Unetched section through a type 303 stainless steel valve exposed to an acidic soft drink in a vending machine. Micrograph shows localized corrosion along manganese sulfide stringer inclusions at the end-grain surface. 100× More
Image
Published: 01 June 2019
Fig. 1 Unetched section through a type 303 stainless steel valve exposed to an acidic soft drink in a vending machine. Micrograph shows localized corrosion along manganese sulfide stringer inclusions at the end-grain surface. 100× More
Image
Published: 15 January 2021
Fig. 33 Unetched section through a type 303 stainless steel valve exposed to an acidic soft drink in a vending machine. Micrograph shows localized corrosion along manganese sulfide stringer inclusions at the end-grain surface. Original magnification: 100× More
Book Chapter

By Brett A. Miller
Series: ASM Handbook Archive
Volume: 11
Publisher: ASM International
Published: 01 January 2002
DOI: 10.31399/asm.hb.v11.a0003501
EISBN: 978-1-62708-180-1
... if dimensioned in some way? Will the available production machines be able to make the part? Production runs Are the desired production runs consistent with the machines and expected costs? Tooling wear Is tooling wear or maintenance a possible problem that will impact part cost or performance...
Book Chapter

Series: ASM Handbook Archive
Volume: 11
Publisher: ASM International
Published: 01 January 2002
DOI: 10.31399/asm.hb.v11.a0003548
EISBN: 978-1-62708-180-1
Book Chapter

By Brett A. Miller
Series: ASM Handbook
Volume: 11A
Publisher: ASM International
Published: 30 August 2021
DOI: 10.31399/asm.hb.v11A.a0006800
EISBN: 978-1-62708-329-4
... and assembly May there be unforeseen difficulties with handling and assembly? Dimensions May the part end up being dimensioned so that assumptions about assembleability become invalid? Tangling May the parts tangle if dimensioned in some way? Will the available production machines be able to make...
Book Chapter

By Michael Cooney, Richard Hoffman
Series: ASM Handbook
Volume: 11
Publisher: ASM International
Published: 15 January 2021
DOI: 10.31399/asm.hb.v11.a0006783