... UNS S45500 Fatigue fracture Stress-corrosion cracking Mechanical springs go into a variety of aerospace systems where both efficiency and reliability are required. Typical applications range from the control of switching characteristics of miniature switches to the deployment of missile fairing...
Series: ASM Failure Analysis Case Histories
Publisher: ASM International
Published: 01 June 2019
DOI: 10.31399/asm.fach.aero.c9001707
EISBN: 978-1-62708-217-4
... (S13800), 15-5 PH (S15500), 17-4 PH (S17400), Custom 450 (S45000), Custom 455(S45500). The martensitic alloys only require a single step heat treatment to obtain maximum strength. Of these alloys, PH 13-8 Mo has often been specified for aerospace applications requiring high strengths (i.e...