... surface embrittlement resulted from oxygen absorption which made the surface layers susceptible to cracking under start up and shutdown. Replacement tubes made of a heat-resistant alloy (e.g., Hastelloy C-276) were recommended. Acicular structure Overheating Tubes ASTM B337 grade 2 UNS R50400...