Series: ASM Failure Analysis Case Histories
Publisher: ASM International
Published: 01 June 2019
DOI: 10.31399/asm.fach.aero.c9001907
EISBN: 978-1-62708-217-4
... bolts Grain flow Carburizing Hy-Tuf UNS K325599 Heat treating related failures Metalworking related failures Stress-corrosion cracking Introduction Component: LAU-7 missile launcher attachment bolts Manufacturing defects: Machining rather than forging/inadvertent carburization...