1-1 of 1 Search Results for

UNS K12320

Follow your search
Access your saved searches in your account

Would you like to receive an alert when new items match your search?
Close Modal
Sort by
Series: ASM Failure Analysis Case Histories
Publisher: ASM International
Published: 01 June 2019
DOI: 10.31399/asm.fach.petrol.c0048830
EISBN: 978-1-62708-228-0
... Pressure vessels Welded joints ASTM A204 grade C UNS K12320 Hydrogen damage and embrittlement Figure 1(a) shows a vessel that had been in service about 3 years as a hydrogen reformer when cracking occurred in the weld between the shell and the lower head. As shown in Detail A in Fig. 1 , one...