.... It was recommended that material that is intended for critical applications where failure cannot be tolerated should be non-destructively examined. Inclusions Pressure vessels Trialefin Tube components ASTM A213 grade T11 UNS K11597 Stress-corrosion cracking After 2 years of service, a return bend...