Series: ASM Failure Analysis Case Histories
Volume: 3
Publisher: ASM International
Published: 01 December 2019
DOI: 10.31399/asm.fach.v03.c9001776
EISBN: 978-1-62708-241-9
... steel) UNS J91149 Introduction Experimental Procedure Results and Discussion Conclusion References References 1. Perry R.H. , Green D.W. : Solid-Solid Operation and Processing, Chemical Engineers’ Handbook , 8th edn. , pp. 56 – 61 . McGraw-Hill , New York ( 2008...