Series: ASM Failure Analysis Case Histories
Volume: 3
Publisher: ASM International
Published: 01 December 2019
DOI: 10.31399/asm.fach.v03.c9001820
EISBN: 978-1-62708-241-9
... cracking. Based on test data and cost, A217-WC9 cast Cr–Mo steel would be a better alloy for the application. valve body corrosion H2S exposure Cr-Mo steel pitting cracks chemical analysis corrosion resistance A216-WCC (cast carbon steel) UNS J02503 A217-WC9 cast Cr–Mo steel UNS K21590...