Series: ASM Failure Analysis Case Histories
Volume: 3
Publisher: ASM International
Published: 01 December 2019
DOI: 10.31399/asm.fach.v03.c9001792
EISBN: 978-1-62708-241-9
... fracture rotary-bending fatigue steel ratchet marks beach marks star-shaped fracture pattern SEM/EDX analysis fatigue strength SAE 4340 (nickel-chromium-molybdenum alloy steel) UNS G43400 SAE 5046H (low-alloy chromium steel) UNS H50460 Introduction Investigation Methodology Results...