Series: ASM Failure Analysis Case Histories
Publisher: ASM International
Published: 01 June 2019
DOI: 10.31399/asm.fach.mech.c0048626
EISBN: 978-1-62708-225-9
... embrittlement 8735 UNS G87350 Surface treatment related failures Hydrogen damage and embrittlement Cadmium-plated high-strength steel bolts were used to facilitate quick disassembly of a vehicle. One bolt was found fractured across the root of a thread after being torqued in place for 1 week. The bolts...