Series: ASM Failure Analysis Case Histories
Publisher: ASM International
Published: 01 June 2019
DOI: 10.31399/asm.fach.auto.c0047846
EISBN: 978-1-62708-218-1
... of shafts was increased to 760 MPA by nitriding for 10 h at 515 deg C. Shock loading Stresses Vibration 8640 UNS G86400 Fatigue fracture The shaft shown in Fig. 1 was from a fuel-injection-pump governor that controlled the speed of a diesel engine used in trucks and tractors. Shafts...