1-1 of 1 Search Results for

UNS G41350

Follow your search
Access your saved searches in your account

Would you like to receive an alert when new items match your search?
Close Modal
Sort by
Series: ASM Failure Analysis Case Histories
Volume: 2
Publisher: ASM International
Published: 01 December 1993
DOI: 10.31399/asm.fach.v02.c9001005
EISBN: 978-1-62708-215-0
... 4135 UNS G41350 Metalworking-related failures Fatigue fracture Background Visual Examination of General Physical Features Testing Procedure and Results Discussion Conclusion and Recommendations Acknowledgments Reference Reference 1. Paul Thielen and Morris Fine, “Fatigue...