... surface imperfections. Electric motors Stress concentration Thermal stresses 1151 UNS G11510 Brittle fracture (Other, general, or unspecified) processing-related failures Splined rotor shafts like that shown in Fig. 1 were used on small electric motors. It was found that one spline...