Series: ASM Failure Analysis Case Histories
Publisher: ASM International
Published: 01 June 2019
DOI: 10.31399/asm.fach.homegoods.c0092135
EISBN: 978-1-62708-222-8
... the barrel walls thicker and more uniform, and/or developing an alternative nontoxic metal shot with a hardness in the range of 30 to 40 HB. Ammunition Guns 1138 UNS G11380 Gross yielding A standard commercial shotgun barrel fabricated from 1138 steel deformed during a test that was made...