EISBN: 978-1-62708-241-9
... metallography stress intensity Al-Si bronze (wrought aluminum-silicon bronze) UNS C64200 Ni-Al bronze (wrought nickel-aluminum bronze) UNS C63200 Introduction The good general corrosion performance of bronze alloys in marine environments is well known [ 1 ], and the combination of strength...