... UNS C51000 Fatigue fracture Premature failure of a copper alloy C51000 (phosphor bronze, 5% A) spring occurred during life testing of several such springs. As shown in Fig. 1(a) , the fracture occurred in bend 2, which had an inside radius of 0.38 mm (0.015 in.). The wire used for the springs...