Series: ASM Failure Analysis Case Histories
Publisher: ASM International
Published: 01 June 2019
DOI: 10.31399/asm.fach.bldgs.c9001697
EISBN: 978-1-62708-219-8
... treatment C12200 UNS C12200 ASTM B88 UNS C12200 Pitting corrosion Potable waters are defined as waters that are suitable for drinking purposes. Potable waters are in use throughout the United States and new systems are being installed on a daily basis. The quality of potable waters...