1-1 of 1 Search Results for

UNS A97049

Follow your search
Access your saved searches in your account

Would you like to receive an alert when new items match your search?
Close Modal
Sort by
Series: ASM Failure Analysis Case Histories
Volume: 2
Publisher: ASM International
Published: 01 December 1993
DOI: 10.31399/asm.fach.v02.c9001292
EISBN: 978-1-62708-215-0
... inspection of the struts was recommended. Crack propagation Fractography Military planes Scanning electron microscopy 7049 UNS A97049 Fatigue fracture Background Visual Examination of General Physical Features Testing Procedure and Results Discussion Conclusion and Recommendations...