Series: ASM Failure Analysis Case Histories
Volume: 1
Publisher: ASM International
Published: 01 December 1992
DOI: 10.31399/asm.fach.v01.c9001124
EISBN: 978-1-62708-214-3
...). The failed cable did not meet either criterion. It was recommended that the replacement cable be inspected for strict compliance to ASTM requirements. Notch sensitivity Welded joints 6201-T81 UNS A96201 Intergranular corrosion Fatigue fracture Background Several wires in aluminum conductor...