Series: ASM Failure Analysis Case Histories
Publisher: ASM International
Published: 01 June 2019
DOI: 10.31399/asm.fach.auto.c9001543
EISBN: 978-1-62708-218-1
... problems. The temperature in much of the piston was high enough to cause softening by overaging, lowering strength. Automotive engines Overheating Pistons Softening 357 UNS A03570 Thermal fatigue fracture Mixed-mode fracture High-temperature corrosion and oxidation The sustained high...