Series: ASM Failure Analysis Case Histories
Publisher: ASM International
Published: 01 June 2019
DOI: 10.31399/asm.fach.homegoods.c9001677
EISBN: 978-1-62708-222-8
... that should be applied when analyzing failures of unknown origin. Fractography Spoons Tableware 420 UNS S42000 Fatigue fracture A good deal of speculation and controversy surrounds the area of paranormal effects on metals. This area caught the public's attention with the emergence of Uri...