... have been eliminated if a killed steel of quality groups 2 or 3 according to DIN 17 100 had been used. Bars Concrete construction Cracking (fracturing) Steelmaking St 34 (Other, general, or unspecified) processing-related failures In a concrete structure a ceiling was hung on flat bars...
Series: ASM Handbook Archive
Volume: 11
Publisher: ASM International
Published: 01 January 2002
DOI: 10.31399/asm.hb.v11.a0001819
EISBN: 978-1-62708-180-1
... prosthesis; metal against metal (G.E.U.P.A.R.). (f) Sliding knee joint prosthesis; metal against plastic (Geomedic). (g) Total shoulder joint prosthesis; metal against plastic (St. Georg). (h) Total finger joint prosthesis with metal and plastic components (St. Georg). (i) Total elbow joint prosthesis; metal...
Series: ASM Failure Analysis Case Histories
Publisher: ASM International
Published: 01 June 2019
DOI: 10.31399/asm.fach.med.c9001690
EISBN: 978-1-62708-226-6
... for institutional support, Z. Panossian (IPT) for helpful comments, G. Spera and A.P. da Silva, the experimental work technicians, T. Puga Leivas (Instituto de Ortopedia e Traumatologia do Hospital das Clínicas) and R. Curtis (Guy's and St. Thomas's Medical and Dental School) for helpful assistance. This work...
Series: ASM Handbook
Volume: 11B
Publisher: ASM International
Published: 15 May 2022
DOI: 10.31399/asm.hb.v11B.a0006924
EISBN: 978-1-62708-395-9
... , 30 ). (Several theoretical treatises of the T g -conversion relationship can be found in Ref 31 to 34 .) As can be seen from the increasing curvature of the data in Fig. 17 , the T g is a more sensitive measure of cure than is conversion, as measured by ΔH res , in the latter stages of cure...
Series: ASM Handbook Archive
Volume: 11
Publisher: ASM International
Published: 01 January 2002
DOI: 10.31399/asm.hb.v11.a0003564
EISBN: 978-1-62708-180-1
... Loading in Transformation-Toughened Ceramics , J. Mech. Phys. Solids , Vol 44 , 1996 , p 207 – 231 10.1016/0022-5096(95)00073-9 29. Tada H. , Paris P.C. , and Irwin G.R. , Stress Analysis of Cracks Handbook , Paris Publications Inc. , St. Louis, MO , 1985 30...
Series: ASM Handbook Archive
Volume: 11
Publisher: ASM International
Published: 01 January 2002
DOI: 10.31399/asm.hb.v11.a0003560
EISBN: 978-1-62708-180-1
Book Chapter

Series: ASM Handbook
Volume: 11
Publisher: ASM International
Published: 15 January 2021
DOI: 10.31399/asm.hb.v11.a0006790
EISBN: 978-1-62708-295-2
Series: ASM Handbook
Volume: 11A
Publisher: ASM International
Published: 30 August 2021
DOI: 10.31399/asm.hb.v11A.a0006810
EISBN: 978-1-62708-329-4
Series: ASM Handbook Archive
Volume: 11
Publisher: ASM International
Published: 01 January 2002
DOI: 10.31399/asm.hb.v11.a0001808
EISBN: 978-1-62708-180-1
Series: ASM Handbook
Volume: 11
Publisher: ASM International
Published: 15 January 2021
DOI: 10.31399/asm.hb.v11.a0006788
EISBN: 978-1-62708-295-2
.... This was ascribed to the air oxidation of some of the sulfide to elemental sulfur, which is extremely corrosive ( Ref 32 – 34 ). On returning to anaerobic conditions, the corrosion rate fell back toward previous levels. Electrical MIC Current thinking distinguishes two basic modes for the direct involvement...
Series: ASM Handbook Archive
Volume: 11
Publisher: ASM International
Published: 01 January 2002
DOI: 10.31399/asm.hb.v11.a0003556
EISBN: 978-1-62708-180-1
... samples and for identifying related MIC sites ( Ref 32 , 33 ). Fungal production of organic acids has been implicated in the corrosion of posttensioned cables used in construction ( Ref 34 ). Fig. 6 Initial corrosion rates for steel exposed to carbonated 3% NaCl solution with 0, 100, and 1000 ppm...
Series: ASM Handbook Archive
Volume: 11
Publisher: ASM International
Published: 01 January 2002
DOI: 10.31399/asm.hb.v11.a0003512
EISBN: 978-1-62708-180-1
Series: ASM Handbook
Volume: 11A
Publisher: ASM International
Published: 30 August 2021
DOI: 10.31399/asm.hb.v11A.a0006808
EISBN: 978-1-62708-329-4
... in the second wire was 34 ppm. Metallurgical Discontinuities Contributing to Weld Rejection and Failures A discontinuity is defined as an interruption of the typical structure of a metal, such as a lack of homogeneity in its mechanical, metallurgical, or physical characteristics. In the context...
Series: ASM Handbook
Volume: 11A
Publisher: ASM International
Published: 30 August 2021
DOI: 10.31399/asm.hb.v11A.a0006831
EISBN: 978-1-62708-329-4
Series: ASM Handbook
Volume: 11B
Publisher: ASM International
Published: 15 May 2022
DOI: 10.31399/asm.hb.v11B.9781627083959
EISBN: 978-1-62708-395-9
Series: ASM Handbook
Volume: 11
Publisher: ASM International
Published: 15 January 2021
DOI: 10.31399/asm.hb.v11.a0006787
EISBN: 978-1-62708-295-2
... end at 95 g/s (750 lb/h), 34 to 69 kPa (5 to 10 psi), and 125 °C (260 °F). The kiln developed perforations within eight months of operation. Sulfur and chlorine in the charcoal attacked the Inconel 601, forming various sulfides and chlorides ( Fig. 7 ). The tendency is for the sulfur to attack...
Series: ASM Handbook
Volume: 11A
Publisher: ASM International
Published: 30 August 2021
DOI: 10.31399/asm.hb.v11A.9781627083294
EISBN: 978-1-62708-329-4
Series: ASM Handbook
Volume: 11A
Publisher: ASM International
Published: 30 August 2021
DOI: 10.31399/asm.hb.v11A.a0006802
EISBN: 978-1-62708-329-4
Series: ASM Handbook
Volume: 11A
Publisher: ASM International
Published: 30 August 2021
DOI: 10.31399/asm.hb.v11A.a0006834
EISBN: 978-1-62708-329-4