Series: ASM Failure Analysis Case Histories
Publisher: ASM International
Published: 01 June 2019
DOI: 10.31399/asm.fach.mech.c9001533
EISBN: 978-1-62708-225-9
... Steam turbines Wear tests Sn-13.5Sb-6.0Cu Sn-11.9Sb-4.5Cu Babbit (Other, miscellaneous, or unspecified) wear 1. Introduction The reliable operation of sliding bearings determines to a considerable extent the life and reliable operation of the steam turbine as a whole. 1 , 2 The cases...