Series: ASM Failure Analysis Case Histories
Volume: 3
Publisher: ASM International
Published: 01 December 2019
DOI: 10.31399/asm.fach.v03.c9001757
EISBN: 978-1-62708-241-9
... steel fatigue cracking microhardness testing hardness STS403 martensitic stainless steel Introduction Background Experimental Procedure Results and Discussion Conclusions Acknowledgments References References 1. Cohen H. , Rogers G.F.C. , Saravanamutto H.I.H...