Series: ASM Failure Analysis Case Histories
Volume: 2
Publisher: ASM International
Published: 01 December 1993
DOI: 10.31399/asm.fach.v02.c9001286
EISBN: 978-1-62708-215-0
... ). An etched view of the disc wall revealed uniform-size grains (average ASTM grain size 8) of mostly ferrite and some pearlite ( Fig. 10 ). Thus, the failed stamped brake disc met the specified AISI-SAE 1015 microstructural requirements. Fig. 8 Typical unetched metallographic cross section of a failed...
Series: ASM Handbook Archive
Volume: 11
Publisher: ASM International
Published: 01 January 2002
DOI: 10.31399/asm.hb.v11.a0001809
EISBN: 978-1-62708-180-1
... (max) MPa psi Solid-metal bearings Aluminum alloy SAE 770-T101 4.1 mm (0.162 in.) thick 34.5 5000 Bimetal bearings Tin babbitt 0.6 mm (0.022 in.) thick on steel 8.3 1200 Lead babbitt 0.6 mm (0.022 in.) thick on steel 9.7 1400 Tin babbitt 0.1 mm (0.004 in.) thick...
Series: ASM Failure Analysis Case Histories
Volume: 3
Publisher: ASM International
Published: 01 December 2019
DOI: 10.31399/asm.fach.v03.c9001763
EISBN: 978-1-62708-241-9
.... splined shaft fatigue fracture transient torsional overloading medium carbon steel spline teeth deformation stress analysis fracture toughness SAE/AISI 1045 (medium-carbon alloy steel) UNS G10450 Introduction Visual Examination Stress Analysis Conclusions References References...
Series: ASM Failure Analysis Case Histories
Volume: 3
Publisher: ASM International
Published: 01 December 2019
DOI: 10.31399/asm.fach.v03.c9001764
EISBN: 978-1-62708-241-9
...Abstract Abstract High failure rates in the drive shafts of 40 newly acquired articulated buses was investigated. The drive shafts were fabricated from a low-carbon (0.45%) steel similar to AISI 5046. Investigators examined all 40 buses, discovering six different drive shaft designs across...
Series: ASM Failure Analysis Case Histories
Volume: 2
Publisher: ASM International
Published: 01 December 1993
DOI: 10.31399/asm.fach.v02.c9001306
EISBN: 978-1-62708-215-0
... A sample of one of the wheel studs was analyzed to check the steel chemical composition. The results are given in Table 1 . This product analysis is consistent with AISI 1541, one of the alloy possibilities mentioned for grade 8.1 wheel studs in SAE Standard J429. Chemical analysis of Grade 8.1 wheel...
Series: ASM Failure Analysis Case Histories
Volume: 3
Publisher: ASM International
Published: 01 December 2019
DOI: 10.31399/asm.fach.v03.c9001759
EISBN: 978-1-62708-241-9
... assembly. drive shaft bearing cup brittle fracture heat treatment carbon steel shallow case endurance and load testing fracture toughness SAE-AISI 1117 (11xx resulfurized steel) UNS G11170 Introduction Problem Statement Analysis of Problem Experimental Procedure Results...
Series: ASM Handbook
Volume: 11A
Publisher: ASM International
Published: 30 August 2021
DOI: 10.31399/asm.hb.v11A.a0006806
EISBN: 978-1-62708-329-4
... to designate these components. The SAE International standards classify thin-walled bearings into three groups: Sleeve-type half-bearings Split-type bushings Thrust washers Based on the previous discussion, it can be said that sliding bearings may also be classified according to material...
Series: ASM Failure Analysis Case Histories
Volume: 3
Publisher: ASM International
Published: 01 December 2019
DOI: 10.31399/asm.fach.v03.c9001792
EISBN: 978-1-62708-241-9
... composition with AISI-SAE designation [ 4 ] Mechanical testing for tensile and fracture properties can provide quantitative measures of strength and susceptibility to failure. Tensile test and Charpy test were conducted to measure the yield strength, percentage of elongation, and the impact energies...
Series: ASM Handbook
Volume: 11A
Publisher: ASM International
Published: 30 August 2021
DOI: 10.31399/asm.hb.v11A.a0006834
EISBN: 978-1-62708-329-4
...–0.60 … … 1–1.20 17.50–18.50 X15CrMoN15 … 0.15–0.30 0.30– 0.80 0.30–0.60 0–0.02 0–0.01 14.5–6.00 0.95–1.10 0–0.30 0.35–0.43 0–0.50 … Corresponding designations of grade AISI 52100 at the international level Table 7 Corresponding designations of grade AISI 52100...
Series: ASM Failure Analysis Case Histories
Volume: 3
Publisher: ASM International
Published: 01 December 2019
DOI: 10.31399/asm.fach.v03.c9001780
EISBN: 978-1-62708-241-9
... on the tool. These properties all lead to less power applied to the machine tool and less heat generation [ 7 ]. The AISI 11xx grades are the common U.S. designations for resulfurized carbon steels, and grade AISI 1144 (~0.44 wt.% carbon) is one of the most common alloys of this type that the analyst...
Series: ASM Handbook
Volume: 11A
Publisher: ASM International
Published: 30 August 2021
DOI: 10.31399/asm.hb.v11A.a0006805
EISBN: 978-1-62708-329-4
... • “ Torque-Tensioning for Inch Series Fasteners ,” SAE J1701-2017, SAE International , 2017 • Wulpi D. , Understanding How Components Fail , 3rd ed. , ASM International , 2013 10.31399/asm.tb.uhcf3.9781627082709 Types of Mechanical Fasteners Fastener Loads Design Load...
Series: ASM Handbook Archive
Volume: 11
Publisher: ASM International
Published: 01 January 2002
DOI: 10.31399/asm.hb.v11.9781627081801
EISBN: 978-1-62708-180-1
Series: ASM Handbook
Volume: 11
Publisher: ASM International
Published: 15 January 2021
DOI: 10.31399/asm.hb.v11.a0006792
EISBN: 978-1-62708-295-2
.... , Determination of Chaboche Combined Hardening Parameters with Dual Backstress for Ratcheting Evaluation of AISI 52100 Bearing Steel , Int. J. Fatigue , Vol 122 , 2019 , p 152 – 163 10.1016/j.ijfatigue.2019.01.009 26. Hahn G.T. , Bhargava V. , and Chen Q. , The Cyclic Stress-Strain...
Series: ASM Handbook Archive
Volume: 11
Publisher: ASM International
Published: 01 January 2002
DOI: 10.31399/asm.hb.v11.a0001812
EISBN: 978-1-62708-180-1
... are necessary as a guide to proper design application and installation. All ASTM and SAE specifications covering threaded fasteners require that the heads be marked for grade identification. Grade markings are a safety device that provides a positive check on selection, use, and inspection. The markings...
Series: ASM Handbook Archive
Volume: 11
Publisher: ASM International
Published: 01 January 2002
DOI: 10.31399/asm.hb.v11.a0003510
EISBN: 978-1-62708-180-1
... for an unalloyed steel (American Iron and Steel Institute, or AISI, 1045) in Fig. 1 . Time-temperature-transformation diagrams can only be read along the isotherms. The temperature A 1 is where transformation to austenite begins, and temperature A 3 is where the transformation to austenite is complete. Fig...
Series: ASM Failure Analysis Case Histories
Volume: 2
Publisher: ASM International
Published: 01 December 1993
DOI: 10.31399/asm.fach.v02.c9001377
EISBN: 978-1-62708-215-0
..., similar to AISI 4140, quenched and tempered to a nominal hardness of 38 to 40 HRC. The chemical analysis and mechanical properties required for this bolt are listed in Tables 1 and 2 . The required minimum tensile strength (1,170 MPa, or 170 ksi) and yield strength (1,050 MPa, or 153 ksi) were somewhat...
Series: ASM Handbook
Volume: 11
Publisher: ASM International
Published: 15 January 2021
DOI: 10.31399/asm.hb.v11.a0006765
EISBN: 978-1-62708-295-2
..., Modified SAE 4620 Steels , Metall. Trans. , Vol 5 , May 1974 , p 1069 – 1085 10.1007/BF02644319 15. Metallography: An Introduction , Metallography and Microstructures , Vol 9 , ASM Handbook , ASM International , 2004 , p 3 – 20 10.31399/asm.hb.v09.a0003720 16. Price C.E...
Series: ASM Handbook
Volume: 11
Publisher: ASM International
Published: 15 January 2021
DOI: 10.31399/asm.hb.v11.a0006759
EISBN: 978-1-62708-295-2
... Engineers (SAE), Aerospace Materials Specifications (AMS), American Iron and Steel Institute (AISI), and military standards (MIL), which can often be tied back to a Unified Numbering System (UNS) designation. Other countries have tailored specifications that must be followed, such as the German Institute...
Series: ASM Failure Analysis Case Histories
Volume: 3
Publisher: ASM International
Published: 01 December 2019
DOI: 10.31399/asm.fach.v03.c9001819
EISBN: 978-1-62708-241-9
... and determination of inclusion contents in stainless steel samples. The average hardness value (HRB 95.48: Table 5 ) is compatible with a 316 AISI-SAE austenitic stainless steel (around HRB 95) [ 16 ]. Hardness values of austenitic steel pump axis Table 5 Hardness values of austenitic steel pump axis...
Series: ASM Handbook
Volume: 11A
Publisher: ASM International
Published: 30 August 2021
DOI: 10.31399/asm.hb.v11A.a0006816
EISBN: 978-1-62708-329-4
... Specification of alloy chemistry (“H” grades) Specification of hardenability (hardness at specific “J” positions on Jominy end quench) Alloy selection Some steel grades prone to macrosegregation of chromium (banding) or gross segregation of manganese (AISI 1340, 1536, 4140H, 4340) Quench...