Series: ASM Failure Analysis Case Histories
Publisher: ASM International
Published: 01 June 2019
DOI: 10.31399/asm.fach.aero.c9001558
EISBN: 978-1-62708-217-4
...Abstract Abstract A liquid hydrogen main fuel control valve for a rocket engine failed by fracture of the Ti-5Al-2.5Sn body during the last of a series of static engine test firings. Fractographic, metallurgical, and stress analyses determined that a combination of fatigue and unexpected...
Series: ASM Failure Analysis Case Histories
Volume: 1
Publisher: ASM International
Published: 01 December 1992
DOI: 10.31399/asm.fach.v01.c9001031
EISBN: 978-1-62708-214-3
... resulted in a higher hot-gas wall temperature and associated degradation of mechanical properties. Combustion chambers Engine components Internal oxidation Pinholes Reentry vehicles Rocket engines Transgranular fracture NARloy-Z High-temperature corrosion and oxidation Brittle fracture...
Series: ASM Handbook
Volume: 11A
Publisher: ASM International
Published: 30 August 2021
DOI: 10.31399/asm.hb.v11A.a0006815
EISBN: 978-1-62708-329-4
... presentation been adequate ( Ref 21 ). Figure 2 shows one such presentation of data, wherein an O-ring damage index for O-ringed rocket engine designs is plotted versus ambient temperature. From visual examination alone, the danger of launching with ambient temperatures below −1 °C (30 °F) is apparent...
Series: ASM Failure Analysis Case Histories
Publisher: ASM International
Published: 01 June 2019
DOI: 10.31399/asm.fach.homegoods.c9001631
EISBN: 978-1-62708-222-8
.... The fisherman pulls once, twice, then three times on the line. The hook fragments and part of the hook careens like a rocket back toward the fisherman. With no time for the fisherman to react, the metal fragment pierces his left eye and embeds in his skull. During examination at the hospital, the doctors...
Series: ASM Handbook
Volume: 11A
Publisher: ASM International
Published: 30 August 2021
DOI: 10.31399/asm.hb.v11A.a0006804
EISBN: 978-1-62708-329-4
.... Note that these do not require the contents to be flammable; steam/water and other nonflammable systems can also result in BLEVEs. Due to the time for the contents to flash to vapor, these events tend to have long durations, on the order of 100 to 1000 ms. Fragment throw and rocketing of vessel pieces...
Series: ASM Handbook Archive
Volume: 11
Publisher: ASM International
Published: 01 January 2002
DOI: 10.31399/asm.hb.v11.a0003502
EISBN: 978-1-62708-180-1
... Fig. 2 Levels of resolution related to the engineering design process. Source: Ref 1 Fig. 3 General sequence of failure investigation from design point of view Fig. 1 Engineering failure set in context. Source: Ref 1 Abstract Abstract This article provides...
Series: ASM Handbook
Volume: 11
Publisher: ASM International
Published: 15 January 2021
DOI: 10.31399/asm.hb.v11.a0006792
EISBN: 978-1-62708-295-2
... Bearing Ceramic Technology Insertion , J. Eng. Gas Turbines Power , Vol 118 ( No. 2 ), 1996 , p 434 – 442 10.1115/1.2816608 122. Nosaka M. and Kikuchi M. , Tribo-Characteristics of Cryogenic Hybrid Ceramic Ball Bearings for Rocket Turbopumps: Bearing Wear and Transfer Film...
Series: ASM Handbook Archive
Volume: 11
Publisher: ASM International
Published: 01 January 2002
DOI: 10.31399/asm.hb.v11.a0003510
EISBN: 978-1-62708-180-1
Series: ASM Handbook Archive
Volume: 11
Publisher: ASM International
Published: 01 January 2002
DOI: 10.31399/asm.hb.v11.a0001818
EISBN: 978-1-62708-180-1
Series: ASM Handbook
Volume: 11A
Publisher: ASM International
Published: 30 August 2021
DOI: 10.31399/asm.hb.v11A.a0006812
EISBN: 978-1-62708-329-4
... If temporary or permanent repairs, physical modifications, or rating (pressure/temperature) changes are needed Satisfying code and regulatory requirements Good engineering and safe work practice considerations. Current risk to other similar equipment could also be identified. Often, the root cause...